Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | TD | ISO294-4 | 0.70to0.90 | % |
Modeling Shrinkage | MD | ISO294-4 | 0.30to0.50 | % |
Moisture Absorption | Equilibrium,23°C,50%RH | ISO62 | 0.16 | % |
Density / Specific Gravity | | ASTMD792 | 1.53 | g/cm³ |
Density / Specific Gravity | | ISO1183 | 1.54 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Stress | Break | ISO527-2/1A/5 | 139 | Mpa |
Tensile Strain | Break | ISO527-2/1A/5 | 2.7 | % |
Tensile Modulus | | ISO527-2/1A/1 | 9200 | Mpa |
Tensile Elongation | Break,23°C | ASTMD638 | 2.8 | % |
Flexural Modulus | 23°C | ISO178 | 8700 | Mpa |
Tensile Strength | Break,23°C | ASTMD638 | 137 | Mpa |
Flexural Stress | 23°C | ISO178 | 210 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Linear thermal expansion coefficient | MD | ISO11359-2 | 2.5E-05 | cm/cm/°C |
Linear thermal expansion coefficient | TD | ISO11359-2 | 1E-04 | cm/cm/°C |
Vicat Softening Temperature | | ISO306/B50 | 220 | °C |
Deflection Temperature Under Load? | 0.45MPa,Unannealed | ISO75-2/B | 225 | °C |
Deflection Temperature Under Load? | 1.8MPa,Unannealed | ISO75-2/A | 205 | °C |
Melting Temperature | | ISO11357-3 | 225 | °C |
Glass Transition Temperature | | ISO11357-2 | 60.0 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Relative Permittivity | 100Hz | IEC60250 | 4.50 | |
Relative Permittivity | 1MHz | IEC60250 | 4.10 | |
Comparative Tracking Index | | IEC60112 | 425 | V |
Surface Resistivity | | IEC60093 | >1.0E+15 | ohms |
Volume Resistivity | | IEC60093 | >1.0E+15 | ohms·cm |
Dissipation Factor? | 100Hz | IEC60250 | 2.2E-03 | |
Dissipation Factor? | 1MHz | IEC60250 | 0.016 | |
Dielectric Strength | | IEC60243-1 | 31 | KV/mm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Notched Izod impact strength | 23°C | ISO180/1U | 35 | kJ/m² |
Charpy Unnotched Impact Strength | -30°C | ISO179/1eU | 45 | kJ/m² |
Charpy Unnotched Impact Strength | 23°C | ISO179/1eU | 46 | kJ/m² |
Charpy Notched Impact Strength | -30°C | ISO179/1eA | 8.5 | kJ/m² |
Charpy Notched Impact Strength | 23°C | ISO179/1eA | 8.5 | kJ/m² |
Notched Izod Impact Strength | 23°C | ISO180/1A | 12 | kJ/m² |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
UL flame retardant rating | 0.70mm | UL94 | HB | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.