Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | MD | ASTMD955 | 1.8到2.0 | % |
Density / Specific Gravity | | ASTMD792 | 1.31 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Strain | Yield | ISO527-2/1A/50 | 4.0 | % |
Tensile Strain | Break | ISO527-2/1A/50 | 30 | % |
Tensile Modulus | | ISO527-2/1A/1 | 2700 | Mpa |
Flexural Modulus | 23°C | ISO178 | 2600 | Mpa |
Flexural Stress | 23°C | ISO178 | 85.0 | Mpa |
Field, 23°C | | ASTMD638 | 57.2 | Mpa |
yield | | ISO527-2/1A/50 | 60.0 | Mpa |
Break,23℃ | | ASTMD638 | 55.8 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
0.45MPa, Unannealed | | ISO75-2/B | 155 | °C |
1.8MPa, Unannealed | | ISO75-2/A | 55.0 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
-- | | ASTMD257 | 1E+16 | ohms·cm |
-- | | IEC60093 | 1E+17 | ohms·cm |
-- | | IEC60243-1 | 15 | KV/mm |
--1 | | ASTMD149 | 17 | KV/mm |
Relative Permittivity | 1MHz | IEC60250 | 3.20 | |
Comparative Tracking Index | | ASTMD3638 | >600 | V |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Charpy Unnotched Impact Strength | 23°C | ISO179/1eU | 100 | kJ/m² |
Charpy Notched Impact Strength | 23°C | ISO179/1eA | 4.0 | kJ/m² |
Notched Izod Impact Strength | 23°C | ISO180/1A | 3.2 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell Hardness | M-Sale | ISO2039-2 | 78 | |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
UL flame retardant rating | | UL94 | HB | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.