PBT SHINITE® D201G30 SHINKONG TAIWAN
176
- Unit Price:
- $2376 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 28.7MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Chemical resistance heat-resisting Electrical performance Filler: Glass fiber reinf 30% filler by weight
- Application Areas:Home appliance components
- Color:--
- Grade:Enhanced level
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD | ASTMD955 | 0.30to1.4 | % |
Moisture Absorption | 23°C,24hr | ASTMD570 | 0.070 | % |
Density / Specific Gravity | ASTMD792 | 1.52 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Compressive Strength | ASTMD695 | 157 | Mpa | |
Tensile Strength | ASTMD638 | 125 | Mpa | |
Tensile Modulus | ASTMD638 | 11900 | Mpa | |
Tensile Elongation | Break | ASTMD638 | 2.2 | % |
Flexural Modulus | ASTMD790 | 8480 | Mpa | |
Flexural Strength | ASTMD790 | 189 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 1.8MPa,Unannealed | ASTMD648 | 208 | °C |
Linear thermal expansion coefficient | MD | ASTMD696 | 3.1E-05 | cm/cm/°C |
Melting temperature | DSC | 224 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dielectric Strength | ASTMD149 | 29 | KV/mm | |
Dielectric Constant | ASTMD150 | 2.20 | ||
Volume Resistivity | ASTMD257 | 1E+16 | ohms·cm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Notched Izod Impact Strength | 3.17mm | ASTMD256 | 91 | J/m |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell Hardness | R-Scale | ASTMD785 | 118 |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | UL94 | HB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.