Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | TD2 | ISO294-4 | 1.5 | % |
Modeling Shrinkage | TD | ISO294-4 | 1.2 | % |
Modeling Shrinkage | MD | ISO294-4 | 0.70 | % |
Modeling Shrinkage | MD2 | ISO294-4 | 0.80 | % |
Moisture Absorption | 23°C,24hr,2.00mm | ISO62 | 0.33 | % |
Moisture Absorption | Equilibrium,23°C,2.00mm,50%RH | ISO62 | 0.14 | % |
MediumDensity | | | 1.37 | g/cm³ |
SpecificHeatCapacityofMelt | | | 1740 | J/kg/°C |
ThermalConductivityofMelt | | | 0.27 | W/m/K |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Flexural Stress | | ISO178 | 155 | Mpa |
Tensile Creep Modulus | 1hr | ISO899-1 | 6000 | Mpa |
Tensile Stress | Break | ISO527-2 | 100 | Mpa |
Tensile Strain | Break | ISO527-2 | 3.4 | % |
Tensile Creep Modulus | 1000hr | ISO899-1 | 4800 | Mpa |
Tensile Modulus | | ISO527-2 | 7200 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Deflection Temperature Under Load? | 0.45MPa,Unannealed | ISO75-2/B | 218 | °C |
Deflection Temperature Under Load? | 1.8MPa,Unannealed | ISO75-2/A | 203 | °C |
Linear thermal expansion coefficient | MD | ISO11359-2 | 5E-05 | cm/cm/°C |
Linear thermal expansion coefficient | TD | ISO11359-2 | 1.1E-04 | cm/cm/°C |
Vicat Softening Temperature | | ISO306/B50 | 207 | °C |
Melting Temperature | | ISO11357-3 | 225 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Dielectric Strength | | IEC60243-1 | 28 | KV/mm |
Relative Permittivity | 100Hz | IEC60250 | 3.70 | |
Relative Permittivity | 1MHz | IEC60250 | 3.50 | |
Comparative Tracking Index | | IEC60112 | 250 | V |
Dissipation Factor? | 100Hz | IEC60250 | 3E-03 | |
Dissipation Factor? | 1MHz | IEC60250 | 0.017 | |
Surface Resistivity | | IEC60093 | 1E+15 | ohms |
Volume Resistivity | | IEC60093 | >1.0E+15 | ohms·cm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Charpy Unnotched Impact Strength | -30°C | ISO179/1eU | 44 | kJ/m² |
Charpy Unnotched Impact Strength | 23°C | ISO179/1eU | 53 | kJ/m² |
Notched Izod impact strength | -30°C | ISO180/1U | 32 | kJ/m² |
Notched Izod impact strength | 23°C | ISO180/1U | 33 | kJ/m² |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
UL flame retardant rating | 0.8mm | IEC60695-11-10,-20 | V-0 | |
UL flame retardant rating | 1.5mm | IEC60695-11-10,-20 | V-0 | |
Oxygen Index | | ISO4589-2 | 31 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.