PBT VALOX™ K4560-BK1066 SABIC INNOVATIVE US
76
- Unit Price:
- $3042 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10.2MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Hydrolysis resistance High mobility Glass fiber reinforced
- Application Areas:Electrical field Electronic field Engine hood parts Automotive External Parts
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:3.20mm | 内部方法 | 0.60to0.80 | % |
TD:3.20mm | 内部方法 | 1.0to1.2 | % | |
Melt Volume flow Rate | 250°C/5.0kg | ISO1133 | 41.0 | cm3/10min |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Elongation | Yield | ASTMD638 | 4.0 | % |
Yield | ASTMD638 | 3.0 | % | |
Break4 | ASTMD638 | 2.5 | % | |
Break | ASTMD638 | 3.0 | % | |
Break | ASTMD638 | 4.0 | % | |
Break7 | ASTMD638 | 2.2 | % | |
Tensile Modulus | ASTMD638 | 8840 | Mpa | |
Tensile Strength | Yield | ASTMD638 | 112 | Mpa |
Tensile Strength | Break3,4 | ASTMD638 | 107 | Mpa |
Break3,5 | ASTMD638 | 115 | Mpa | |
Break3,6 | ASTMD638 | 110 | Mpa | |
Break3 | ASTMD638 | 112 | Mpa | |
Break3,7 | ASTMD638 | 102 | Mpa | |
Break8,7 | ASTMD638 | 96.0 | Mpa | |
Flexural Modulus | 50.0mmSpan5 | ASTMD790 | 7100 | Mpa |
50.0mmSpan6 | ASTMD790 | 7500 | Mpa | |
50.0mmSpan4 | ASTMD790 | 8000 | Mpa | |
50.0mmSpan | ASTMD790 | 7200 | Mpa | |
50.0mmSpan7 | ASTMD790 | 7400 | Mpa | |
Flexural Strength | Break,50.0mmSpan | ASTMD790 | 173 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 0.45MPa,Unannealed,3.20mm | ASTMD648 | 220 | °C |
1.8MPa,Unannealed,3.20mm | ASTMD648 | 200 | °C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Instrumented Dart Impact | 23°C,TotalEnergy4 | ASTMD3763 | 6.10 | J |
23°C,TotalEnergy5 | ASTMD3763 | 7.56 | J | |
23°C,TotalEnergy7 | ASTMD3763 | 8.81 | J |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.