PPO FLEX NORYL™ WCP761 BK1006 SABIC INNOVATIVE US
74
- Unit Price:
- $3852 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Low Specific Gravity Low water absorption Non enhanced
- Application Areas:Wire insulation applicati
- Color:--
- Grade:--
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Moisture Absorption | 23°C,24hr | ASTMD570 | 0.10 | % |
Melt Mass-Flow Rate | 210°C/5.0kg | ASTMD1238 | 15 | g/10min |
250°C/2.16kg | ASTMD1238 | 20 | g/10min | |
Modeling Shrinkage | MD:24hr | ASTMD955 | 1.1 | % |
TD:24hr | ASTMD955 | 1.1 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Elongation | Break | ASTMD638 | 170 | % |
Tensile Strength | Break | ASTMD638 | 7.50 | Mpa |
Flexural Modulus | 100mmSpan | ASTMD790 | 50.0 | Mpa |
ISO178 | 40.0 | Mpa | ||
Tensile Stress | Break | ISO527-2/50 | 8.00 | Mpa |
Tensile Strain | Break | ISO527-2/50 | 170 | % |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Brittleness Temperature | ASTMD746 | <-40.0 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dissipation Factor? | 1MHz | IEC60250 | 2E-03 | |
Relative Permittivity | 1MHz | IEC60250 | 2.50 | |
Comparative Tracking Index | IEC60112 | 600 | V | |
Electric strength | 2.00mm,inOil | IEC60243-1 | 25 | KV/mm |
Volume Resistivity | ASTMD257 | 1.3E+16 | ohms·cm |
Film | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tearing Strength | ISO6383-1 | 16.0 | N/mm |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shore Hardness | Shore A,30sec | ASTMD2240 | 78 |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Oxygen Index | ISO4589-2 | 24 | % | |
Glow Wire Ignition Temperature | 3.0mm | IEC60695-2-13 | 775 | °C |
UL flame retardant rating | 6.0mm | UL94 | V-0 | |
Glow Wire Flammability Index | 3.0mm | IEC60695-2-12 | 960 | °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.