PPS INFINO® XP-2130A Samsung Cheil South Korea
126
- Unit Price:
- $5814 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 22.5MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:enhance Flame retardant Filler: Glass fiber reinf
- Application Areas:Connector Automotive Applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:3.20mm | ASTMD955 | 0.30to1.2 | % |
TD:3.20mm | ASTMD955 | 0.30to1.2 | % | |
TD:3.20mm | ISO2577 | 0.30to1.2 | % | |
MD:3.20mm | ISO2577 | 0.30to1.2 | % | |
Ash Content | -- | ISO3451 | 30 | % |
-- | ASTMD5630 | 30 | % | |
Melt Mass-Flow Rate | 315°C/5.0kg | ASTMD1238 | 120 | g/10min |
315°C/5.0kg | ISO1133 | 120 | g/10min | |
Density / Specific Gravity | ASTMD792 | 1.65 | g/cm³ | |
ISO1183 | 1.65 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flexural Modulus | ASTMD790 | 9800 | Mpa | |
ISO178 | 10000 | Mpa | ||
Flexural Stress | ISO178 | 190 | Mpa | |
Tensile Modulus | ASTMD638 | 5900 | Mpa | |
Tensile Strength | Break | ASTMD638 | 130 | Mpa |
Yield | ASTMD638 | 140 | Mpa | |
Tensile Elongation | Break | ASTMD638 | 3.0 | % |
Flexural Strength | ASTMD790 | 200 | Mpa | |
Tensile Stress | Break | ISO527-2/5 | 115 | Mpa |
Yield | ISO527-2/5 | 128 | Mpa | |
Tensile Strain | Break | ISO527-2/5 | 3.0 | % |
Tensile Modulus | ISO527-2/5 | 8000 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 0.45MPa,Unannealed,6.40mm | ASTMD648 | 282 | °C |
0.45MPa,Unannealed,4.00mm | ISO75-2/B | 289 | °C | |
1.8MPa,Unannealed,6.40mm | ASTMD648 | 275 | °C | |
1.8MPa,Unannealed,4.00mm | ISO75-2/A | 275 | °C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO179/1eA | 11 | kJ/m² |
Notched Izod Impact Strength | 23°C | ISO180/1A | 11 | kJ/m² |
Notched Izod Impact Strength | 23°C,3.18mm | ASTMD256 | 88 | J/m |
23°C,6.35mm | ASTMD256 | 79 | J/m |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell Hardness | R-Scale | ASTMD785 | 120 | |
R-Scale | ISO2039-2 | 116 |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flame Rating | 0.75mm | UL94 | V-0 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.