Material Description
Technical Data Sheet
Material Description
- Material Properties:dimensional stability High rigidity Filler: Glass mineral
- Application Areas:--
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Density | ASTM D792/ISO 1183 | 1.96 | ||
Moisture Absorption 23℃/24H | ASTM D570/ISO 62 | 0.02 | % |
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD | ASTMD955 | 0.15 | % |
TD | ASTMD955 | 0.45 | % | |
Moisture Absorption | 24hr | ASTMD570 | 0.020 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Modulus | ASTM D638/ISO 527 | 22*10^4 | kg/cm²(MPa)[Lb/in²] | |
ASTMD638 | 21600 | Mpa | ||
Tensile Strength | ASTM D638/ISO 527 | 1730 | kg/cm²(MPa)[Lb/in²] | |
Tensile Elongation | Break | ASTMD638 | 1.4 | % |
Flexural Modulus | ASTMD790 | 18600 | Mpa | |
ASTM D790/ISO 178 | 19*10^4 | kg/cm²(MPa)[Lb/in²] | ||
Flexural Strength | ASTM D790/ISO 178 | 2390 | kg/cm²(MPa)[Lb/in²] | |
Yield | ASTMD790 | 234 | Mpa | |
Tensile Strength | Yield | ASTMD638 | 170 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Linear thermal expansion coefficient | MD | ASTMD696 | 1.2E-05 | cm/cm/°C |
TD | ASTMD696 | 4.8E-05 | cm/cm/°C | |
Deflection Temperature Under Load? | ASTM D648/ISO 75 | >260 | ℃(℉) | |
1.8MPa,Unannealed | ASTMD648 | 260 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dissipation Factor? | 1kHz | ASTMD150 | 0.055 | |
1MHz | ASTMD150 | 8.5E-03 | ||
Dielectric Constant | 1kHz | ASTMD150 | 5.10 | |
1MHz | ASTMD150 | 4.50 | ||
Arc Resistance | ISO 14782 | 137 | ||
ASTMD495 | 137 | sec | ||
Volume Resistivity | ASTMD257 | 1E+15 | ohms·cm | |
Dielectric Strength | ASTMD149 | 11 | KV/mm | |
Comparative Tracking Index | IEC60112 | 215 | V |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell Hardness | R-Scale | ASTMD785 | 121 |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | UL94 | V-0 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.