Technical Data Sheet
Physical properties | Test Condition | Test Method | Test Result | Unit |
---|
density | | ASTM D792/ISO 1183 | 1.66 | |
Water absorption rate 23 ℃/24h | | ASTM D570/ISO 62 | 0.01 | % |
physical property | Test Condition | Test Method | Test Result | Unit |
---|
Water absorption rate | 23°C,24hr | ISO62 | 0.030 | % |
Melt viscosity | 310°C,1000sec^-1 | ISO11443 | 380000 | mPa·s |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|
Bending stress | | ISO178 | 260 | Mpa |
Tensile stress | | ISO527-2 | 185 | Mpa |
Tensile strain | Break | ISO527-2 | 1.8 | % |
tensile strength | | ASTM D638/ISO 527 | 185 | kg/cm²(MPa)[Lb/in²] |
Bending modulus | | ASTM D790/ISO 178 | 13000 | kg/cm²(MPa)[Lb/in²] |
Bending modulus | | ISO178 | 1300 | Mpa |
bending strength | | ASTM D790/ISO 178 | 260 | kg/cm²(MPa)[Lb/in²] |
Tensile elongation at break (elongation at break) | | ASTM D638/ISO 527 | 1.8 | % |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|
Combustibility (rate) | | UL94 | V-0 | |
Hot deformation temperature | 1.8MPa,Unannealed | ISO75-2/A | 265 | °C |
Linear coefficient of thermal expansion | MD | 内部方法 | 1E-05 | cm/cm/°C |
Linear coefficient of thermal expansion | TD | 内部方法 | 4E-05 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Volume resistivity | | ASTM D257/IEC 60093 | 1.0 x 10^16 | Ω.cm |
Volume resistivity | | IEC60093 | 1E+16 | ohms·cm |
Dissipation factor | 1kHz | IEC60250 | 2E-03 | |
Dissipation factor | 1MHz | IEC60250 | 2E-03 | |
Dissipation factor | 耐电弧性 | IEC60250 | 120 | sec |
Dielectric strength | 3.00mm | IEC60243-1 | 15 | KV/mm |
Relative permittivity | 1kHz | IEC60250 | 4.60 | |
Relative permittivity | 1MHz | IEC60250 | 4.60 | |
Leakage Trace Index | | IEC60112 | 150 | V |
Processing performance | Test Condition | Test Method | Test Result | Unit |
---|
Mold temperature | | | 150 | °C |
Processing temperature | | | 290-300 | °C |
Processing temperature | | | 310 | °C |
Processing temperature | | | 300 | °C |
Processing temperature | | | 310-320 | °C |
Dry conditions | | | 160℃3H | |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell hardness | M-Scale | ISO2039-2 | 105 | |
flammability | Test Condition | Test Method | Test Result | Unit |
---|
UL flame retardant rating | | UL94 | V-0 | |
Supplementary Information | Test Condition | Test Method | Test Result | Unit |
---|
ColourNumber | | | HF2000/HD9050 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.