PPS Torelina® A504 TORAY JAPAN
199
- Unit Price:
- $5814 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 105MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:high strength Glass fiber reinforced enhance Flame retardant High rigidity
- Application Areas:Electrical applications Lighting fixtures
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
density | ASTM D792/ISO 1183 | 1660 | ||
Water absorption rate 23 ℃/24h | ASTM D570/ISO 62 | 0.02 | % |
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | Flow | 东丽法 | 0.20 | % |
垂重方向 | 东丽法 | 0.70 | % | |
Flowing Long | 320℃,98MPa,1mm厚 | 东丽法 | 124 |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
abrasion | ASTM D-1044 | 50 | mg/1000回 | |
Limit PV value | 东丽法 | 东丽法 | KJ/m | |
Curved elastic body | ASTM D-790 | 13.7 | GPa | |
hardness | ASTM D-785 | 120 | 洛氏 | |
Fracture strength | ASTM D-732 | 75 | ||
Tensile strength | ASTM D-638 | 155 | Mpa | |
friction coefficient | 对钢 | ASTM D-1894 | 0.25 | |
impact strength | Notched23℃ | ASTM D-256 | 100 | J/m |
Unnotched23℃ | ASTM D-256 | 30 | KJ/m | |
tensile strength | ASTM D638/ISO 527 | 165 | kg/cm²(MPa)[Lb/in²] | |
ASTM D-638 | 1.6 | % | ||
elongation | ASTM D638/ISO 527 | 1.4 | % | |
Rockwell hardness | ASTM D785 | R-123 | ||
bending strength | ASTM D790/ISO 178 | 250 | kg/cm²(MPa)[Lb/in²] | |
ASTM D-790 | 205 | Mpa | ||
Charpy impact strength | ASTM D256/ISO 179 | 30 | kg·cm/cm(J/M)ft·lb/in |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Combustibility | UL-94 | V-0 | ||
Combustibility (rate) | UL94 | V-0 (0.28mmt) | ||
Hot deformation temperature | ASTM D648/ISO 75 | >260 | ℃(℉) | |
1.82MPa | ASTM D-648 | >260 | °C | |
Rongdian | DSC | 278 | °C | |
Line expansion coefficient | Flow | ASTM D-696 | 2.2 | |
垂重方向 | ASTM D-696 | 3.3 |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Arc resistance W level | ASTM D-495 | 127 | 秒 | |
permittivity | 10 | ASTM D-150 | 3.8 | |
Induced positive connection | 10 | ASTM D-150 | 0.002 | |
Inherent resistance of volume | ASTM D-257 | 10 | Ω.m | |
Insulation breakdown voltage | ASTM D-149 | 21 | MV/m | |
Dielectric constant | ASTM D150/IEC 60250 | 3.6 | ||
Volume resistivity | ASTM D257/IEC 60093 | 10^14 | Ω.cm |
Basic performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Water absorption rate | ASTM D-570 | 0.02 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.