LCP VECTRA® A435-NC-VF3001 CELANESE USA
41
- Unit Price:
- $6244 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 50MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Flame retardant enhance Glass fiber reinforced
- Application Areas:Home appliance components Automotive Applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | TD | ISO294-4 | 0.40 | % |
MD | ISO294-4 | 0.10 | % | |
Moisture Absorption | Equilibrium,23°C,50%RH | ISO62 | 2E-03 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Stress | Break | ISO527-2/1A/5 | 171 | Mpa |
Tensile Strain | Break | ISO527-2/1A/5 | 3.3 | % |
Tensile Modulus | ISO527-2/1A/1 | 11000 | Mpa | |
Flexural Modulus | 23°C | ISO178 | 10500 | Mpa |
Flexural Stress | 23°C | ISO178 | 206 | Mpa |
Compressive Modulus | ISO604 | 10500 | Mpa | |
CompressiveStress | 1%Strain | ISO604 | 77.0 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Vicat Softening Temperature | ISO306/B50 | 146 | °C | |
Melting Temperature | ISO11357-3 | 280 | °C | |
Deflection Temperature Under Load? | 0.45MPa,Unannealed | ISO75-2/B | 250 | °C |
1.8MPa,Unannealed | ISO75-2/A | 230 | °C | |
8.0MPa,Unannealed | ISO75-2/C | 162 | °C | |
Linear thermal expansion coefficient | MD | ISO11359-2 | 1E-06 | cm/cm/°C |
TD | ISO11359-2 | 1.9E-05 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dissipation Factor? | 100Hz | IEC60250 | 0.020 | |
1MHz | IEC60250 | 0.016 | ||
Surface Resistivity | IEC60093 | >1.0E+15 | ohms | |
Arc Resistance | 内部方法 | 130 | sec | |
Volume Resistivity | IEC60093 | 1E+15 | ohms·cm | |
Relative Permittivity | 100Hz | IEC60250 | 3.50 | |
1MHz | IEC60250 | 3.10 | ||
Comparative Tracking Index | IEC60112 | 175 | V | |
Dielectric Strength | IEC60243-1 | 32 | KV/mm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Notched Izod impact strength | 23°C | ISO180/1U | 33 | kJ/m² |
Charpy Unnotched Impact Strength | 23°C | ISO179/1eU | 38 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell Hardness | M-Scale | ISO2039-2 | 55 |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | UL94 | V-0 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.