PC/ABS WONDERLOY® PC-365KB ZHENJIANG CHIMEI
72
- Unit Price:
- $2512 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Flame retardant heat-resisting High impact resistance
- Application Areas:Electrical applications Automotive Applications currency
- Color:--
- Grade:--
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD | ASTMD955 | 0.40to0.60 | % |
ISO2577 | 0.40to0.60 | % | ||
Melt Mass-Flow Rate | 260°C/5.0kg | ASTMD1238 | 20 | g/10min |
260°C/5.0kg | ISO1133 | 20 | g/10min | |
SpiralFlow3,4 | 内部方法 | 30.0 | CM |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Stress | Yield | ISO527-2/50 | 54.0 | Mpa |
Break | ISO527-2/50 | 50.0 | Mpa | |
Tensile Strain | Break | ISO527-2/50 | 120 | % |
Flexural Modulus | 23°C | ASTMD790 | 2260 | Mpa |
Tensile Strain | Break,23°C | ASTMD638 | 85 | % |
Flexural Modulus | ISO178 | 2200 | Mpa | |
Flexural Strength | 23°C | ASTMD790 | 78.5 | Mpa |
Tensile Strength | Yield,23°C | ASTMD638 | 53.0 | Mpa |
Flexural Stress | ISO178 | 80.0 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Heat Deflection Temperature | 1.8MPa,Unannealed,3.20mm | ASTMD648 | 106 | °C |
1.8MPa,Unannealed,6.40mm | ASTMD648 | 115 | °C | |
1.8MPa,Unannealed,4.00mm | ISO75-2/A | 102 | °C | |
Linear thermal expansion coefficient | MD:23to55°C | ISO11359-2 | 8E-05 | cm/cm/°C |
MD:-40to40°C | ASTME831 | 8E-05 | cm/cm/°C | |
Vicat Softening Temperature | -- | ASTMD152510 | 136 | °C |
-- | ASTMD152511 | 125 | °C | |
-- | ISO306/A50 | 138 | °C | |
-- | ISO306/B50 | 127 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Surface Resistivity | IEC60093 | 1E+16 | ohms | |
Dielectric Constant | 1MHz | IEC60250 | 3.10 | |
Volume Resistivity | IEC60093 | 1E+18 | ohms·cm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Notched Izod Impact Strength | -30°C | ISO180 | 45 | kJ/m² |
23°C | ISO180 | 50 | kJ/m² | |
Charpy Notched Impact Strength | -30°C | ISO179 | 45 | kJ/m² |
23°C | ISO179 | 50 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell Hardness | R-Sale,23°C | ASTMD785 | 115 | |
R-Sale,23°C | ISO2039-2 | 115 |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 1.5mm | UL94 | HB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.