PC/ABS INFINO®  NH-1045 Samsung Cheil South Korea

109
  • Unit Price:
    $3374 USD/MT
  • Packaging Specification:
    25 KG/PKG
  • Supply Quantity:
    36.5MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:Flame retardant
  • Application Areas:sporting facilities
  • Color:--
  • Grade:High liquidity level

Technical Data Sheet

physical property Test ConditionTest MethodTest ResultUnit
Shrinkage rateFlow : 3.20 mmASTM D9550.40 到 0.70%
Shrinkage rateAcross Flow : 3.20 mmASTM D9550.40 到 0.70%
Shrinkage rateAcross Flow : 2.00 mmISO 294-40.40 到 0.70%
Shrinkage rate流量 : 2.00 mmISO 294-40.40 到 0.70%
Melt flow rate220°C/10.0 kgASTM D1238, ISO 113355g/10 min
Mechanical performanceTest ConditionTest MethodTest ResultUnit
Tensile modulus-- 3ASTM D6382500Mpa
Tensile modulus--ISO 527-2/502500Mpa
elongationBreak 3ASTM D63850%
elongationBreakISO 527-2/5050%
Bending modulus-- 4ASTM D7902600Mpa
Bending modulus-- 5ISO 1782600Mpa
bending strength -- 4ASTM D79091.0Mpa
bending strength -- 5ISO 17893.0Mpa
Tensile strengthYield 3ASTM D63862.0Mpa
Tensile strengthYieldISO 527-2/5063.0Mpa
Tensile strengthBreak 3ASTM D63844.0Mpa
Tensile strengthBreakISO 527-2/5045.0Mpa
Thermal performanceTest ConditionTest MethodTest ResultUnit
Vicat softening temperatureISO 306/B5095.0°C
Thermal deformation temperature under load0.45 MPa, Unannealed, 6.40 mmASTM D64888.0°C
Thermal deformation temperature under load0.45 MPa, Unannealed, 4.00 mmISO 75-2/B88.0°C
Thermal deformation temperature under load1.8 MPa, Unannealed, 6.40 mmASTM D64880.0°C
Thermal deformation temperature under load1.8 MPa, Unannealed, 4.00 mmISO 75-2/A78.0°C
injectionTest ConditionTest MethodTest ResultUnit
Temperature at the rear of the barrel230 到 270°C
Temperature in the middle of the barrel240 到 280°C
Temperature at the front of the material cylinder250 到 290°C
Spray nozzle temperature250 到 290°C
Back pressure0.981 到 2.94Mpa
Screw speed50 到 200rpm
Injection pressure98.1Mpa
Hot air dryer4.0hr
Hot air dryer80°C
Vacuum drying machine80°C
Vacuum drying machine4.0hr
Suggested maximum moisture content0.020%
Mold temperature60 到 80°C
hardnessTest ConditionTest MethodTest ResultUnit
Rockwell hardnessR-ScaleASTM D785116
Rockwell hardnessR -SaleISO 2039-2116
flammabilityTest ConditionTest MethodTest ResultUnit
UL flame retardant rating1.5 to 3.0 mmUL 94V-0
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.