PC/ABS Bayblend® T45 COVESTRO GERMANY
178
- Unit Price:
- $3497 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Easy electroplating
- Application Areas:Electrical tools Electrical field Electronic field Household appliances Household appliances Automotive sector
- Color:--
- Grade:Flame retardant grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Moisture Absorption | Saturation,23°C | ISO62 | 0.70 | % |
Equilibrium,23°C,50%RH | ISO62 | 0.20 | % | |
Melt Volume flow Rate | 260°C/5.0kg | ISO1133 | 12.0 | cm3/10min |
Density / Specific Gravity | 23°C | ISO1183 | 1.10 | g/cm³ |
Melt Viscosity | 260°C | ISO11443-A | 200 | Pa·s |
Modeling Shrinkage | TD:260°C,3.00mm | ISO2577 | 0.55to0.75 | % |
MD:260°C,3.00mm | ISO2577 | 0.55to0.75 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Stress | Yield,23°C | ISO527-2/50 | 49.0 | Mpa |
Break,23°C | ISO527-2/50 | 40.0 | Mpa | |
Tensile Strain | Yield,23°C | ISO527-2/50 | 3.7 | % |
Break,23°C | ISO527-2/50 | >50 | % | |
Tensile Modulus | 23°C | ISO527-2/1 | 2100 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 0.45MPa,Unannealed | ISO75-2/B | 112 | °C |
1.8MPa,Unannealed | ISO75-2/A | 95.0 | °C | |
Linear thermal expansion coefficient | TD:23to55°C | ISO11359-2 | 9E-05 | cm/cm/°C |
MD:23to55°C | ISO11359-2 | 8.5E-05 | cm/cm/°C | |
Vicat Softening Temperature | -- | ISO306/B50 | 110 | °C |
-- | ISO306/B120 | 112 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Relative Permittivity | 23°C,100Hz | IEC60250 | 3.10 | |
23°C,1MHz | IEC60250 | 3.00 | ||
Comparative Tracking Index | SolutionA | IEC60112 | 275 | V |
Dielectric Strength | 23°C,1.00mm | IEC60243-1 | 35 | KV/mm |
Surface Resistivity | IEC60093 | 1E+16 | ohms | |
Volume Resistivity | 23°C | IEC60093 | 1E+16 | ohms·cm |
Dissipation Factor? | 23°C,100Hz | IEC60250 | 3.5E-03 | |
23°C,1MHz | IEC60250 | 8.5E-03 |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Notched Izod impact strength | -30°C | ISO180 | NoBreak | |
23°C | ISO180 | NoBreak | ||
Notched Izod Impact Strength | -30°C | ISO180/A | 36 | kJ/m² |
23°C | ISO180/A | 40 | kJ/m² |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flame Rating | 0.9mm | UL94 | HB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.