PC/ABS LNP™ THERMOCOMP™ NX10302 SABIC INNOVATIVE NANSHA
76
- Unit Price:
- $6593 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 60.1MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High mobility Flame retardant
- Application Areas:Electrical applications Lighting fixtures
- Color:--
- Grade:Halogen-free flame retardant grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD3.20mm | ASTMD995 | 0.60-0.65 | % |
TD3.20mm | ASTMD995 | 0.50-0.56 | % | |
Moisture Absorption | (23°C,24hr) | ASTMD570 | 0.010 | % |
吸湿性 | ASTMD570 | 0.0200 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Notched Izod Impact Strength | 23°C | ASTMD256 | 600 | J/m |
悬壁梁Unnotched冲击强度 | ASTMD4812 | NB | J/m | |
Tensile Elongation?(Break) | Yield,5mm/min,23°C | ASTMD638 | 4.2 | % |
5mm/min,23°C | ASTMD638 | 100 | % | |
Tensile Modulus | 50mm/min,23°C | ASTMD638 | 2480 | Mpa |
Tensile Strength | Yield,5mm/min,23°C | ASTMD638 | 46.0 | Mpa |
5mm/min,23°C | ASTMD638 | 47.0 | Mpa | |
Flexural Modulus | 1.3mm/min,23°C | ASTMD790 | 2400 | Mpa |
Flexural Strength | Yield,1.3mm/min,23°C | ASTMD790 | 80.0 | Mpa |
1.3mm/min,23°C | ASTMD790 | 79.0 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 1.80MPaUnannealed | ASTMD648 | 108 | °C |
Coefficient of Linear Thermal Expansion | MD | ASTMD696 | 8.47E-05 | cm/cm/°C |
TD | ASTMD696 | 9.1E-05 | cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.