Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Moulding shrinkage | | ASTM D-9 | 4-6 | in/in× |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Strength(Yield) | 2.0in/min | ASTM D-6 | 5800 | psi |
Tensile Elongation?(Yield) | 2.0in/min | ASTM D-6 | 5.0 | % |
Tensile Strength (Yield) | | ASTM D-7 | 15000 | psi |
Tensile Modulus | 2.0in/min | ASTM D-6 | 390000 | psi |
Tensile Elongation?(Break) | 2.0in/min | ASTM D-6 | 50.0 | % |
IZOD Notch Impact Strength | | IS0 13477 | 11.0 | ft-lb/in |
Shore Hardness | | ASTM D-7 | 120 | R scale |
Instrumented Dart Impact | | TMA | 600 | in-lbs |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
HDT | 264PSi | ASTM D-6 | 210 | |
HDT | 66PSi | ASTM D-6 | 229 | |
CTE | | ASTM E-8 | 4×10 | in/in-F |
Thermal Conductivity | | ISO 75-2/Bf | 0.20 | W/m-c |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Temperature Index | 电性能 | UL 746B | 90 | degC |
Temperature Index | 机械冲击能量 | UL 746B | 80 | degC |
Temperature Index | 非机械冲击能量 | UL 746B | 90 | degC |
Dielectric Strength | 125mils | ASTM D-1 | 457 | v/mil |
Surface Resistivity | | IS0 13477 | >1×10 | Ω/sq |
Dielectric Constant | 50Hz | ASTM D-1 | 3.00 | |
Dielectric Constant | 100Hz | ASTM D-1 | 3.00 | v/mil |
Volume Resistivity | | IS0 13477 | 1×10 | Ω.cm |
Dissipation Factor | 50Hz | ASTM D-1 | 0.0048 | |
Physical | Test Condition | Test Method | Test Result | Unit |
---|
Melt index | | ASTM D-1 | 16.0 | g/10min |
Moisture Absorption | | N.m | 0.40 | % |
Moisture Absorption | 24hr | N.m | 0.100 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.