PC LEXAN™ 1000R SABIC INNOVATIVE NANSHA
68
- Unit Price:
- $2551 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 60.5MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:wear resistant High impact resistance High mobility
- Application Areas:Electrical field Electronic field Automotive sector
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:3.20mm | 内部方法 | 0.50to0.70 | % |
Moisture Absorption | 24hr | ASTMD570 | 0.25 | % |
Equilibrium,23°C | ASTMD570 | 1.3 | % | |
Melt Mass-Flow Rate | 337°C/6.6kg | ASTMD1238 | 9.7 | g/10min |
Density / Specific Gravity | ASTMD792 | 1.27 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flexural Strength | Yield,100mmSpan | ASTMD790 | 165 | Mpa |
Taber Abrasion Resistance | 1000Cycles,1000g,CS-17Wheel | ASTMD1044 | 10.0 | mg |
Poisson Ratio | ASTMD638 | 0.36 | ||
Tensile Elongation | Yield | ASTMD638 | 7.0 | % |
Tensile Modulus | ASTMD638 | 3590 | Mpa | |
Tensile Strength | Yield | ASTMD638 | 110 | Mpa |
Flexural Modulus | 100mmSpan | ASTMD790 | 3520 | Mpa |
Tensile Elongation | Break | ASTMD638 | 60 | % |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Thermal Conductivity | ASTMC177 | 0.22 | W/m/K | |
RTIElec | UL746 | 170 | °C | |
Evolution Calendar intelligent importer | UL746 | 170 | °C | |
RTIStr | UL746 | 170 | °C | |
Deflection Temperature Under Load? | 0.45MPa,Unannealed,6.40mm | ASTMD648 | 210 | °C |
1.8MPa,Unannealed,6.40mm | ASTMD648 | 201 | °C | |
Linear thermal expansion coefficient | MD:-20to150°C | ASTME831 | 5.6E-05 | cm/cm/°C |
TD:-20to150°C | ASTME831 | 5.4E-05 | cm/cm/°C | |
Vicat Softening Temperature | ASTMD15255 | 219 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dielectric Strength | 1.60mm,inAir | ASTMD149 | 33 | KV/mm |
1.60mm,in Oil | ASTMD149 | 28 | KV/mm | |
Dielectric Constant | 1kHz | ASTMD150 | 3.15 | |
Volume Resistivity | ASTMD257 | 1E+17 | ohms·cm | |
Dissipation Factor? | 1kHz | ASTMD150 | 1.3E-03 | |
2.45GHz | ASTMD150 | 2.5E-03 | ||
Arc Resistance | ASTMD495 | PLC5 | ||
Comparative Tracking Index | CTI | UL746 | PLC4 | |
Hot-wire Ignition | HWI | UL746 | PLC1 | |
High Amp Arc Ignition | HAI | UL746 | PLC3 | |
High Voltage Arc Tracking Rate | HVTR | UL746 | PLC2 |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Gardner Impact | 23°C | ASTMD3029 | 36.6 | J |
Reverse Notch Izod Impact | 3.20mm | ASTMD256 | 1600 | J/m |
Notched Izod Impact Strength | 23°C | ASTMD256 | 53 | J/m |
23°C | ASTMD4812 | 1300 | J/m |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell Hardness | M-Scale | ASTMD785 | 109 |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Oxygen Index | ASTMD2863 | 47 | % | |
UL flame retardant rating | 0.40mm | UL94 | V-2 | |
0.75mm | UL94 | V-0 | ||
3.0mm | UL94 | 5VA | ||
NBSSmokeDensity-Flaming,Ds,4min | ASTME662 | 0.700 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.