PC LNP™ LUBRICOMP™ DFL-34 BK1A657L SABIC INNOVATIVE US
63
- Unit Price:
- $2554 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Easy to form Easy to demould
- Application Areas:Electronic and Electrical Lighting applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:24hr | ASTMD955 | 0.020到0.040 | % |
TD:24hr | ASTMD955 | 0.20到0.40 | % | |
24hr,50%RH | ASTMD570 | 0.090 | % | |
Equilibrium,23°C,50%RH | ISO62 | 0.13 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Break | ASTMD638 | 95.0 | Mpa | |
Break,50.0mm Span | ASTMD790 | 145 | Mpa | |
--1 | ASTMD638 | 7190 | Mpa | |
yield | ISO527-2/5 | 2.8 | % | |
fracture | ISO527-2/5 | 3.1 | % | |
ISO527-2/5 | 93.0 | Mpa | ||
Coefficient of Friction | Itself - Dynamic | ASTMD3702Modified | 0.46 | |
Itself - Static | ASTMD3702Modified | 0.50 | ||
Specific Wear Rate | Ring | ASTMD3702Modified | 13.0 | 10^-10in^5-min/ft-lb-hr |
Washer | ASTMD3702Modified | 89.0 | 10^-10in^5-min/ft-lb-hr | |
Break | ASTMD638 | 2.7 | % | |
50.0mm Span | ASTMD790 | 6320 | Mpa | |
--5 | ISO178 | 6200 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
0.45MPa, Unannealed,3.20mm Span | ISO75-2/Bf | 146 | °C | |
1.8MPa, Unannealed,3.20mm | ASTMD648 | 142 | °C | |
1.8MPa, Unannealed,64.0mm Span | ISO75-2/Af | 141 | °C | |
0.45MPa, Unannealed,3.20mm | ASTMD648 | 146 | °C | |
Linear thermal expansion coefficient | MD:-30to30°C | ASTMD696 | 3.7E-05 | cm/cm/°C |
TD:-30to30°C | ASTMD696 | 6.3E-05 | cm/cm/°C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
-- | ISO6603-2 | 6.60 | J | |
23°C | ASTMD256 | 150 | J/m | |
ASTMD4812 | 740 | J/m | ||
23°C,TotalEnergy | ASTMD3763 | 19.6 | J | |
23°C7 | ISO180/1A | 14 | kJ/m² | |
23°C8 | ISO180/1U | 49 | kJ/m² |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.