PC LEXAN™ EXL1414 WH9A240 SABIC INNOVATIVE NANSHA
84
- Unit Price:
- $3374 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 23MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Processability Moderate liquidity Ductility copolymer Good demolding performanc
- Application Areas:Electrical applications Home appliance components Fitness equipment
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:3.20mm | 内部方法 | 0.40to0.80 | % |
TD:3.20mm | 内部方法 | 0.40to0.80 | % | |
Moisture Absorption | Saturation,23°C | ISO62 | 0.35 | % |
Equilibrium,23°C,50%RH | ISO62 | 0.15 | % | |
Melt Mass-Flow Rate | 300°C/1.2kg | ASTMD1238 | 10 | g/10min |
Melt Volume flow Rate | 300°C/1.2kg | ISO1133 | 9.00 | cm3/10min |
Density / Specific Gravity | ASTMD792 | 1.18 | g/cm³ | |
ISO1183 | 1.19 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Elongation | Yield | ASTMD638 | 6.0 | % |
Flexural Strength | ISO178 | 85.0 | Mpa | |
Tensile Elongation | Break | ASTMD638 | 98 | % |
Flexural Modulus | ISO178 | 2250 | Mpa | |
Tensile Modulus | ASTMD638 | 2020 | Mpa | |
Tensile Strength | Break | ASTMD638 | 50.3 | Mpa |
Yield | ASTMD638 | 55.5 | Mpa | |
Flexural Modulus | 50.0mmSpan | ASTMD790 | 2230 | Mpa |
Flexural Strength | Yield,50.0mmSpan | ASTMD790 | 92.4 | Mpa |
Tensile Stress | Yield | ISO527-2/50 | 57.0 | Mpa |
Break | ISO527-2/50 | 60.0 | Mpa | |
Tensile Strain | Yield | ISO527-2/50 | 6.0 | % |
Break | ISO527-2/50 | 120 | % | |
Tensile Modulus | ISO527-2/1 | 2150 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 0.45MPa,Unannealed,3.20mm | ASTMD648 | 139 | °C |
1.8MPa,Unannealed,3.20mm | ASTMD648 | 124 | °C | |
Linear thermal expansion coefficient | MD:-40to40°C | ASTME831 | 7E-05 | cm/cm/°C |
MD:23to80°C | ISO11359-2 | 7.2E-05 | cm/cm/°C | |
TD:-40to40°C | ASTME831 | 7.5E-05 | cm/cm/°C | |
TD:23to80°C | ISO11359-2 | 7.2E-05 | cm/cm/°C | |
RTIElec | UL746 | 130 | °C | |
Evolution Calendar intelligent importer | UL746 | 120 | °C | |
RTIStr | UL746 | 125 | °C | |
Ball PressureTest | 125°C | IEC60695-10-2 | Pass | |
Vicat Softening Temperature | ASTMD152510 | 145 | °C | |
-- | ISO306/B50 | 145 | °C | |
-- | ISO306/B120 | 146 | °C | |
Heat Deflection Temperature | 1.8MPa,Unannealed,100mmSpan | ISO75-2/Ae | 128 | °C |
0.45MPa,Unannealed,100mmSpan | ISO75-2/Be | 140 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dissipation Factor? | 100Hz | ASTMD150 | 1.2E-03 | |
1MHz | ASTMD150 | 9.3E-03 | ||
Dielectric Strength | 0.800mm,inOil | ASTMD149 | 16 | KV/mm |
Surface Resistivity | ASTMD257 | >1.0E+15 | ohms | |
Dielectric Constant | 100Hz | ASTMD150 | 2.68 | |
1MHz | ASTMD150 | 2.64 | ||
Volume Resistivity | ASTMD257 | >1.0E+15 | ohms·cm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Unnotched Izod Impact Strength | -30°C | ISO180/1U | NoBreak | |
23°C | ISO180/1U | NoBreak | ||
Instrumented Dart Impact | 23°C,TotalEnergy | ASTMD3763 | 70.0 | J |
Charpy Notched Impact Strength | -30°C | ISO179/1eA | 65 | kJ/m² |
23°C | ISO179/1eA | 70 | kJ/m² | |
Charpy Unnotched Impact Strength | -30°C | ISO179/1eU | NoBreak | |
23°C | ISO179/1eU | NoBreak | ||
Notched Izod Impact Strength | -30°C | ISO180/1A | 60 | kJ/m² |
23°C | ISO180/1A | 70 | kJ/m² | |
Notched Izod Impact Strength | -30°C | ASTMD256 | 770 | J/m |
23°C | ASTMD256 | 870 | J/m |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell Hardness | L-Sale | ASTMD785 | 89 | |
R-Sale | ASTMD785 | 121 |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Glow Wire Ignition Temperature | 1.0mm | IEC60695-2-13 | 875 | °C |
3.0mm | IEC60695-2-13 | 875 | °C | |
UL flame retardant rating | 0.40mm | UL94 | HB | |
Glow Wire Flammability Index | 0.8mm | IEC60695-2-12 | 850 | °C |
1.0mm | IEC60695-2-12 | 960 | °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.