PC LEXAN™ HP4-1H111 SABIC INNOVATIVE US
80
- Unit Price:
- $5344 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High mobility
- Application Areas:medicine Medical/nursing supplies medical care
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:3.20mm | 内部方法 | 0.50to0.70 | % |
Moisture Absorption | 24hr | ASTMD570 | 0.15 | % |
Equilibrium,23°C | ASTMD570 | 0.35 | % | |
Equilibrium,100°C | ASTMD570 | 0.58 | % | |
Melt Mass-Flow Rate | 300°C/1.2kg | ASTMD1238 | 11 | g/10min |
Melt Volume flow Rate | 300°C/1.2kg | ISO1133 | 10.0 | cm3/10min |
Specific Volume | ASTMD792 | 0.830 | cm³/g |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flexural Modulus | ISO178 | 2300 | Mpa | |
Flexural Strength | ISO178 | 90.0 | Mpa | |
Tensile Elongation | Break | ASTMD638 | 130 | % |
Taber Abrasion Resistance | 1000Cycles,1000g,CS-17Wheel | ASTMD1044 | 10.0 | mg |
Tensile Elongation | Yield | ASTMD638 | 7.0 | % |
Tensile Modulus | ASTMD638 | 2370 | Mpa | |
Tensile Strength | Break | ASTMD638 | 68.0 | Mpa |
Yield | ASTMD638 | 62.0 | Mpa | |
Flexural Modulus | 50.0mmSpan | ASTMD790 | 2340 | Mpa |
Flexural Strength | Yield,50.0mmSpan | ASTMD790 | 97.0 | Mpa |
Tensile Stress | Yield | ISO527-2/50 | 63.0 | Mpa |
Break | ISO527-2/50 | 70.0 | Mpa | |
Tensile Strain | Yield | ISO527-2/50 | 6.0 | % |
Break | ISO527-2/50 | 110 | % | |
Tensile Modulus | ISO527-2/1 | 2350 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 0.45MPa,Unannealed,6.40mm | ASTMD648 | 137 | °C |
1.8MPa,Unannealed,6.40mm | ASTMD648 | 132 | °C | |
Vicat Softening Temperature | ASTMD152510 | 154 | °C | |
-- | ISO306/A50 | 153 | °C | |
-- | ISO306/B50 | 141 | °C | |
-- | ISO306/B120 | 142 | °C | |
Linear thermal expansion coefficient | MD:-40to95°C | ASTME831 | 6.8E-05 | cm/cm/°C |
MD:23to80°C | ISO11359-2 | 7E-05 | cm/cm/°C | |
RTIElec | UL746 | 130 | °C | |
Evolution Calendar intelligent importer | UL746 | 130 | °C | |
RTIStr | UL746 | 130 | °C | |
Specific Heat | ASTMC351 | 1250 | J/kg/°C | |
Thermal Conductivity | ASTMC177 | 0.19 | W/m/K | |
ISO8302 | 0.20 | W/m/K | ||
Ball PressureTest | 125°C | IEC60695-10-2 | Pass | |
Heat Deflection Temperature | 1.8MPa,Unannealed,100mmSpan | ISO75-2/Ae | 125 | °C |
0.45MPa,Unannealed,100mmSpan | ISO75-2/Be | 136 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot-wire Ignition | HWI | UL746 | PLC2 | |
Comparative Tracking Index | CTI | UL746 | PLC2 | |
High Amp Arc Ignition | HAI | UL746 | PLC1 | |
High Voltage Arc Tracking Rate | HVTR | UL746 | PLC2 | |
Relative Permittivity | 50Hz | IEC60250 | 2.70 | |
60Hz | IEC60250 | 2.70 | ||
1MHz | IEC60250 | 2.70 | ||
Dissipation Factor? | 50Hz | ASTMD150 | 9E-04 | |
60Hz | ASTMD150 | 9E-04 | ||
1MHz | ASTMD150 | 0.010 | ||
50Hz | IEC60250 | 1E-03 | ||
60Hz | IEC60250 | 1E-03 | ||
1MHz | IEC60250 | 0.010 | ||
Dielectric Strength | 3.20mm,inAir | ASTMD149 | 15 | KV/mm |
3.20mm,in Oil | IEC60243-1 | 17 | KV/mm | |
Surface Resistivity | IEC60093 | >1.0E+15 | ohms | |
Dielectric Constant | 1MHz | ASTMD150 | 2.96 | |
50Hz | ASTMD150 | 3.17 | ||
60Hz | ASTMD150 | 3.17 | ||
Volume Resistivity | ASTMD257 | >1.0E+17 | ohms·cm | |
IEC60093 | >1.0E+15 | ohms·cm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Instrumented Dart Impact | 23°C,EnergyatPeakLoad | ASTMD3763 | 63.0 | J |
Gardner Impact | 23°C | ASTMD3029 | 169 | J |
Notched Izod Impact Strength | -30°C | ISO180/1A | 10 | kJ/m² |
23°C | ISO180/1A | 12 | kJ/m² | |
Tensile Impact Strength | ASTMD1822 | 577 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell Hardness | M-Sale | ASTMD785 | 70 | |
R-Sale | ASTMD785 | 118 |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Refractive index of light | ASTMD542 | 1.586 | ||
Haze | 2540µm | ASTMD1003 | 1.0 | % |
Transmittance | 2540µm | ASTMD1003 | 88.0 | % |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 1.5mm | UL94 | HB | |
Oxygen Index | ASTMD2863 | 25 | % | |
ISO4589-2 | 25 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.