PC PANLITE® G-3110H TEIJIN JAPAN
80
- Unit Price:
- $3005 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 23MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Flame retardant transparent
- Application Areas:Mechanical parts with req Electrical applications electrical equipment Electronic components Lighting fixtures
- Color:--
- Grade:Flame retardant grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Transmittance | 厚度3mm | ASTM D-1003 | 半透明 | % |
Rockwell Hardness | ASTM D-785 | 86 | M标度 |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Compressive Strength | ASTM D-695 | 109(1110) | MPa(Kgf/cm | |
Notched Izod Impact Strength | 艾氏、带Notched厚度3.2mm | ASTM D-256 | 90(9) | J/m(kgf·cm/cm) |
艾氏、带Notched厚度6.4mm | ASTM D-256 | 90(9) | J/m(kgf·cm/cm) | |
Tensile Modulus | ASTM D-638 | 4120(42000) | MPa(Kgf/cm | |
Tensile Strength | Break点 | ASTM D-638 | 83(850) | MPa(Kgf/cm |
Flexural Modulus | ASTM D-790 | 3530(36000) | MPa(Kgf/cm | |
Flexural Strength | ASTM D-790 | 132(1350) | MPa(Kgf/cm |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Coefficient of Linear Thermal Expansion | Flow | ASTM D-696 | 4.0 | |
Across Flow | ASTM D-696 | 6.7 | ||
Heat Deflection Temperature | 负荷1.813MPa(18.6kgf/cm) | ASTM D-648 | 146 | °C |
负荷0.451MPa(4.6kgf/cm) | ASTM D-648 | 150 | °C | |
Temperature Index | 电学式,厚度1.47mm | UL 746B | 130 | °C |
冲击式,厚度1.47mm | UL 746B | 120 | °C | |
非冲击式,厚度1.47mm | UL 746B | 130 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Insulation failure strength | 快速加压值厚度1.6mm | ASTM D-149 | 30 | KV/mm |
Dissipation Factor (Tangent) | 60Hz | ASTM D-150 | 0.0008 | |
10 | ASTM D-150 | 0.009 | ||
Comparative Tracking Index | IEC 112 | 180 | V | |
Dielectric Constant | 10 | ASTM D-150 | 3.07 | |
60Hz | ASTM D-150 | 3.16 | ||
Arc Resistance | ASTM D-495 | 100 | sec | |
Volume Resistivity | ASTM D-257 | 1 |
Processing | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | Flow | ASTM D-955 | 0.3~0.5 | % |
Across Flow | ASTM D-955 | 0.4~0.6 | % |
Physical | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Moisture Absorption | 24hr,in 23℃ | ASTM D-570 | 0.16 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.