PC LEXAN™ GLX143-NA9C029H SABIC INNOVATIVE US
82
- Unit Price:
- $5893 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Middle flow Thermal stability
- Application Areas:Electronic display Application in the automo Lighting applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD1 | 内部方法 | 0.50到0.70 | % |
Moisture Absorption | Saturation,23°C | ISO62 | 0.35 | % |
Equilibrium,23°C,50%RH | ISO62 | 0.15 | % | |
Melt Volume flow Rate | 300°C/1.2kg | ISO1133 | 12.0 | cm3/10min |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flexural Stress | ISO178 | 90.0 | Mpa | |
Tensile Stress | Yield | ISO527-2/50 | 65.0 | Mpa |
Break | ISO527-2/50 | 70.0 | Mpa | |
Tensile Strain | Yield | ISO527-2/50 | 6.0 | % |
Break | ISO527-2/50 | 120 | % | |
Tensile Modulus | ISO527-2/1 | 2350 | Mpa | |
Flexural Modulus | ISO178 | 2300 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Linear thermal expansion coefficient | MD:23to80°C | ISO11359-2 | 7E-05 | cm/cm/°C |
TD:23to80°C | ISO11359-2 | 7E-05 | cm/cm/°C | |
RTIElec | UL746 | 130 | °C | |
Evolution Calendar intelligent importer | UL746 | 125 | °C | |
Thermal Conductivity | ISO8302 | 0.20 | W/m/K | |
RTI | UL746 | 125 | °C | |
Ball PressureTest | 125°C | IEC60695-10-2 | Pass | |
1.8MPa, Unannealed,64.0mm Span | ISO75-2/Af | 124 | °C | |
-- | ISO306/B50 | 142 | °C | |
ISO306/B120 | 143 | °C | ||
0.45MPa, Unannealed,100mm Span | ISO75-2/Be | 136 | °C | |
1.8MPa, Unannealed,100mm Span | ISO75-2/Ae | 125 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Relative Permittivity | 50Hz | IEC60250 | 2.70 | |
60Hz | IEC60250 | 2.70 | ||
1MHz | IEC60250 | 2.70 | ||
Dissipation Factor? | 50Hz | IEC60250 | 1E-03 | |
60Hz | IEC60250 | 1E-03 | ||
1MHz | IEC60250 | 0.010 | ||
Dielectric Strength | 1.00mm11 | IEC60243-1 | 15 | KV/mm |
3.20mm,in Oil | IEC60243-1 | 17 | KV/mm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Unnotched Impact Strength | -30°C | ISO179/1eU | 无断裂 | |
23°C | ISO179/1eU | 无断裂 | ||
Notched Izod Impact Strength | -30°C | ISO180/1A | 12 | kJ/m² |
23°C | ISO180/1A | 70 | kJ/m² | |
Unnotched Izod Impact Strength | -30°C | ISO180/1U | 无断裂 | |
23°C | ISO180/1U | 无断裂 | ||
Charpy Notched Impact Strength | -30°C | ISO179/1eA | 14 | kJ/m² |
23°C | ISO179/1eA | 73 | kJ/m² |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Haze | 2540µm | ASTMD1003 | <0.80 | % |
Refractive index of light | ISO489 | 1.586 | ||
Transmittance | 3000µm | ASTMD1003 | 89.0 | % |
4000µm | ASTMD1003 | 88.0 | % | |
5000µm | ASTMD1003 | 87.0 | % | |
6000µm | ASTMD1003 | 86.0 | % |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Glow Wire Flammability Index | 1.00mm | IEC60695-2-12 | 850 | °C |
Oxygen Index | ISO4589-2 | 25 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.