PC LEXAN™ 4701R SABIC INNOVATIVE US
87
- Unit Price:
- $5483 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 61.1MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High temperature resistan transparent
- Application Areas:Electronic and electrical
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:3.20mm | 内部方法 | 0.80to1.0 | % |
Moisture Absorption | 24hr | ASTMD570 | 0.19 | % |
Melt Mass-Flow Rate | 300°C/1.2kg | ASTMD1238 | 2.0 | g/10min |
300°C/6.1kg | ASTMD1238 | 9.0 | g/10min | |
Specific Volume | ASTMD792 | 0.830 | cm³/g | |
Density | ASTMD792 | 1.19 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Strength | 屈服 | ASTMD638 | 65.5 | Mpa |
断裂 | ASTMD638 | 77.9 | Mpa | |
Tensile Elongation | 断裂 | ASTMD638 | 78 | % |
Flexural Modulus | 50.0mm跨距 | ASTMD790 | 2330 | Mpa |
Flexural Strength | 屈服,50.0mm跨距 | ASTMD790 | 97.2 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 1.8MPa,未退火,3.20mm | ASTMD648 | 149 | °C |
RTIElec | UL746 | 130 | °C | |
Evolution Calendar intelligent importer | UL746 | 130 | °C | |
RTIStr | UL746 | 130 | °C | |
Linear thermal expansion coefficient | MD:-40到95°C | ASTME831 | 8.1E-05 | cm/cm/°C |
Specific Heat | ASTMC351 | 1260 | J/kg/°C | |
Thermal Conductivity | ASTMC177 | 0.21 | W/m/K |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dielectric Strength | 3.20mm,inAir | ASTMD149 | 20 | KV/mm |
Volume Resistivity | ASTMD257 | >2.5E+17 | ohms·cm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Impact Strength | ASTMD1822 | 578 | kJ/m² | |
Gardner Impact | 23°C | ASTMD3029 | 149 | J |
Notched Izod Impact Strength | 23°C | ASTMD256 | 370 | J/m |
23°C | ASTMD4812 | 3200 | J/m |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Transmittance | 2540µm | ASTMD1003 | 85.0 | % |
Haze | 2540µm | ASTMD1003 | 1.0 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.