Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | Across Flow : 2.00 mm | 内部方法 | 0.50 到 0.70 | % |
Modeling Shrinkage | 流量 : 2.00 mm | 内部方法 | 0.50 到 0.70 | % |
Moisture Absorption | Equilibrium, 23°C, 50% RH | ISO 62 | 0.23 | % |
Melt Volume flow Rate | 300°C/1.2 kg | ISO 1133 | 65.0 | cm3/10min |
Density | | ISO 1183 | 1.20 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Flexural Modulus | | ISO 178 | 2300 | Mpa |
Tensile Stress | Yield | ISO 527-2 | 65.0 | Mpa |
Flexural Stress | | ISO 178 | 90.0 | Mpa |
Nominal Tensile Strain at Break | | ISO 527-2 | 80 | % |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
RTI | | UL 746 | 80.0 | °C |
RTI Imp | | UL 746 | 80.0 | °C |
RTI Elec | | UL 746 | 80.0 | °C |
Deflection Temperature Under Load? | 1.8 MPa, Unannealed | ISO 75-2/A | 127 | °C |
Coefficient of Linear Thermal Expansion (Flow) | | ISO 11359-2 | 6.5E-5 | cm/cm/°C |
Injection | Test Condition | Test Method | Test Result | Unit |
---|
Drying Temperature | | | 120 | °C |
Mold Temperature | | | 80 到 120 | °C |
Drying Time | | | 5.0 到 8.0 | hr |
Rear Temperature | | | 240 到 260 | °C |
Middle Temperature | | | 240 到 260 | °C |
Front Temperature | | | 240 到 260 | °C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Charpy Notched Impact Strength | 23°C | ISO 179 | 15 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell Hardness | M -Sale | ISO 2039-2 | 50 | |
Rockwell Hardness | R -Sale | ISO 2039-2 | 120 | |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|
ISO Shortname | | | >PC< | |
Refractive index of light | | ASTM D542 | 1.585 | |
Transmittance | | ISO 13468-1 | 90.0 | % |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
Flame Rating | 0.40 mm, NC | UL 94 | V-2 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.