Material Description
Technical Data Sheet
Material Description
- Material Properties:High mobility
- Application Areas:Food containers
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD | ASTMD955 | 0.50to0.70 | % |
MD | ISO294-4 | 0.50to0.70 | % | |
Moisture Absorption | 23°C,24hr | ASTMD570 | 0.15 | % |
23°C,24hr | ISO62 | 0.15 | % | |
Equilibrium,23°C,50%RH | ASTMD570 | 0.32 | % | |
Equilibrium,23°C,50%RH | ISO62 | 0.32 | % | |
Melt Mass-Flow Rate | 300°C/1.2kg | ASTMD1238 | 22 | g/10min |
300°C/1.2kg | ISO1133 | 22 | g/10min | |
Melt Mass-Flow Rate | 300°C/1.2kg | ISO11332 | 18.0 | cm3/10min |
Density / Specific Gravity | ASTMD792 | 1.20 | g/cm³ | |
ISO1183/A | 1.20 | g/cm³ | ||
ISO11832 | 1200 | kg/m3 |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Nominalstrainatbreak | ISO527-22 | >50 | % | |
Flexural Stress | ISO178 | 97.0 | Mpa | |
Tensile Strength | Yield | ASTMD638 | 60.0 | Mpa |
Break | ASTMD638 | 65.5 | Mpa | |
Flexural Modulus | ASTMD790 | 2410 | Mpa | |
Flexural Strength | ASTMD790 | 96.5 | Mpa | |
Tensile Elongation | Break | ASTMD638 | 120 | % |
Flexural Modulus | ISO178 | 2400 | Mpa | |
Tensile Modulus | ASTMD638 | 2340 | Mpa | |
Taber Abrasion Resistance | ASTMD1044 | 45 | % | |
Tensile Stress | Yield | ISO527-2/50 | 60.0 | Mpa |
Yield | ISO527-22 | 60.0 | Mpa | |
Break | ISO527-2/50 | 66.0 | Mpa | |
Tensile Strain | Yield | ISO527-22 | 6.0 | % |
Break | ISO527-2/50 | 120 | % | |
Tensile Modulus | ISO527-2/50 | 2300 | Mpa | |
ISO527-22 | 2300 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 1.8MPa | ISO75-22 | 128 | °C |
0.45MPa,Unannealed | ISO75-2/B | 139 | °C | |
0.45MPa,Annealed | ASTMD648 | 142 | °C | |
0.45MPa,Annealed | ISO75-2/B | 142 | °C | |
0.45MPa | ISO75-22 | 142 | °C | |
1.8MPa,Unannealed | ASTMD648 | 126 | °C | |
1.8MPa,Annealed | ASTMD648 | 139 | °C | |
1.8MPa,Annealed | ISO75-2/A | 126 | °C | |
Linear thermal expansion coefficient | MD:-40to82°C | ASTMD696 | 6.8E-05 | cm/cm/°C |
MD | ISO11359-22 | 7E-05 | cm/cm/°C | |
Ball Indentation Temperature | IEC60335-1 | 125 | °C | |
Vicat Softening Temperature | ASTMD15257 | 147 | °C | |
ISO306/B50 | 147 | °C | ||
50N | ISO3062 | 147 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Electric strength | IEC60243-12 | 17 | KV/mm | |
Relative Permittivity | 100Hz | IEC602502 | 3.00 | |
1MHz | IEC602502 | 3.00 | ||
Comparative Tracking Index | 2.00mm,SolutionA | IEC60112 | 250 | V |
Dielectric Strength | ASTMD149 | 17 | KV/mm | |
IEC60243-1 | 17 | KV/mm | ||
Dissipation Factor? | 50Hz | ASTMD150 | 1E-03 | |
1MHz | ASTMD150 | 2E-03 | ||
100Hz | IEC602502 | 1E-03 | ||
1MHz | IEC602502 | 2E-03 | ||
Dielectric Constant | 60Hz | ASTMD150 | 3.00 | |
1MHz | ASTMD150 | 3.00 | ||
Volume Resistivity | ASTMD257 | 2E+17 | ohms·cm | |
IEC600932 | >1.0E+13 | ohms·m |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Notched Izod impact strength | 23°C | ISO180 | NoBreak | |
Tensile Impact Strength | ASTMD1822 | 378 | kJ/m² | |
CharpyNotchedImpactStrength | 23°C | ISO179/1eA2 | 70.0 | kJ/m² |
Charpy impact strength | 23°C | ISO179/1eU2 | NoBreak | |
Charpy Notched Impact Strength | -30°C | ISO179/1eU2 | NoBreak | |
Charpy Notched Impact Strength | -30°C | ISO179/1eA2 | 11.0 | kJ/m² |
Notched Izod Impact Strength | 23°C | ASTMD256 | 750 | J/m |
23°C | ISO180/A | 74 | kJ/m² | |
23°C | ASTMD256 | NoBreak | ||
InstrumentedDartImpact6 | 23°C,TotalEnergy | ASTMD3763 | 72.3 | J |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell Hardness | M-Sale | ASTMD785 | 72 | |
R-Sale | ASTMD785 | 118 |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Refractive index of light | ASTMD542 | 1.586 | ||
ISO489 | 1.586 | |||
Haze | ASTMD1003 | 1.0 | % | |
Transmittance | ASTMD1003 | 89.0 | % |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Average Extent of Burning | ASTMD635 | 3 | CM | |
Flame Rating | 1.6mm | UL94 | HB | |
3.2mm | UL94 | HB | ||
Oxygen Index | ISO4589-2 | 26 | % | |
BurningBehav.at1.6mmnom.thickn. | 1.60mm,UL | ISO12102 | HB | |
Burning Behav.atthicknessh | 3.20mm,UL | ISO12102 | HB | |
Oxygenindex | ISO4589-22 | 26 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.