Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Melt Mass-Flow Rate | | ASTM D1238/ISO 1133 | 11 300℃ 1.2KG | g/10min |
Density | | ASTM D792/ISO 1183 | 1220 | |
Moisture Absorption 23℃/24H | | ASTM D570/ISO 62 | 0.2 | % |
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Transmittance | 厚度3mm | ASTM D-1003 | 半透明 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Elongation (Break) | 50mm/min | ISO 527-1 and ISO 527-2 | >50 | % |
Tensile Stress(Yield) | 50mm/min | ISO 527-1 and ISO 527-2 | 62 | Mpa |
Tensile Elongation?(Yield) | 50mm/min | ISO 527-1 and ISO 527-2 | 6 | % |
Compressive Strength | | ASTM D-695 | 78(800) | MPa(Kgf/cm |
Izod Impact Strength | 带Notched | ISO 179 | 12 | KJ/m |
Izod Impact Strength | 没Notched | ISO 179 | NB | KJ/m |
Tensile Modulus | | ASTM D638/ISO 527 | 2400 | kg/cm²(MPa)[Lb/in²] |
Tensile Modulus | 1mm/min | ISO 527-1 and ISO 527-2 | 2400 | Mpa |
Tensile Strength | | ASTM D638/ISO 527 | 62 | kg/cm²(MPa)[Lb/in²] |
Tensile Elongation | | ASTM D638/ISO 527 | 6 | % |
Flexural Modulus | | ASTM D790/ISO 178 | 2200 | kg/cm²(MPa)[Lb/in²] |
Flexural Modulus | 2mm/min | ISO 178 | 2200 | Mpa |
Flexural Strength | 2mm/min | ISO 178 | 90 | Mpa |
Flexural Strength | | ASTM D790/ISO 178 | 90 | kg/cm²(MPa)[Lb/in²] |
Tensile Elongation?(Break) | | ASTM D638/ISO 527 | >50 | % |
Charpy impact strength | | ASTM D256/ISO 179 | 12 | kg·cm/cm(J/M)ft·lb/in |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Coefficient of Linear Thermal Expansion | Flow | ISO 11359-2 | 0.7 | |
Coefficient of Linear Thermal Expansion | Across Flow | ISO 11359-2 | 0.7 | |
Burning Rate | | UL94 | V-0 | |
Vicat Softening Temperature | 50℃/h 50N | ISO 308 | 148 | °C |
Temperature Index | 电学式,厚度1.47mm | UL 746B | 125 | °C |
Temperature Index | 冲击式,厚度1.47mm | UL 746B | 115 | °C |
Temperature Index | 非冲击式,厚度1.47mm | UL 746B | 125 | °C |
Deflection Temperature Under Load | 1.80MPa | ISO 75-1 and ISO 75-2 | 129 | °C |
Deflection Temperature Under Load | 0.45MPa | ISO 75-1 and ISO 75-2 | 141 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Surface Resistivity | | ASTM D257/IEC 60093 | >1x10^15 | Ω |
Surface Resistivity | | IEC 60093 | >1×10 | Ω |
Dielectric Constant | 100Hz | IEC 60250 | 3.1 | |
Dielectric Constant | 1MHz | IEC 60250 | 3 | |
Dielectric Constant | | ASTM D150/IEC 60250 | 3.1 | |
Dielectric Constant | | ASTM D150/IEC 60250 | 3 | |
Arc Resistance | | IEC 60112 | 275 | |
Volume Resistivity | | ASTM D257/IEC 60093 | >1x10^13 | Ω.cm |
Volume Resistivity | | IEC 60093 | >1×10 | Ω.cm |
Arc Resistance | 短时间法 | IEC 60243-1 | 30 | KV/m |
Dissipation Factor?(Tangent) | 100Hz | IEC 60250 | 10 | |
Dissipation Factor?(Tangent) | 1MHz | IEC 60250 | 90 | |
Dielectric loss | | ASTM D150/IEC 60250 | 10 | |
Dielectric loss | | ASTM D150/IEC 60250 | 90 | |
Processing | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | Flow | 本公司制订的测定法 | 0.5~0.7 | % |
Modeling Shrinkage | Across Flow | 本公司制订的测定法 | 0.5~0.7 | % |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|
Transmittance | | ASTM D1003/ISO 13468 | 半透明 | % |
Physical | Test Condition | Test Method | Test Result | Unit |
---|
Moisture Absorption | 放置23°C水中24hr | ISO 62 | 0.2 | % |
Density | | ISO 1183 | 1220 | kg/m |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.