PC PANLITE® K-1300Y TEIJIN JAPAN
146
- Unit Price:
- $3554 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 101MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:transparent
- Application Areas:Translucent accessories film sheet Cleaning Compound transparent
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Density | ASTM D792/ISO 1183 | 1200 | ||
Modeling Shrinkage | ASTM D955 | 0.5~0.7 | % | |
Moisture Absorption 23℃/24H | ASTM D570/ISO 62 | 0.2 | % |
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | TD:4.00mm | 内部方法 | 0.50to0.70 | % |
MD:4.00mm | 内部方法 | 0.50to0.70 | % | |
0.5-0.7 | % | |||
Moisture Absorption | 23℃,24hrs | ISO 62 | 0.2 | % |
23°C,24hr | ISO62 | 0.20 | % | |
Melt Volume flow Rate | 300°C/1.2kg | ISO1133 | 2.80 | cm3/10min |
Melt Volume flow Rate | ISO 1133 | 2.5 | CM |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Nominal Tensile Strain at Break | ISO527-2/50 | >50 | % | |
Tensile Elongation?(Yield) | ISO 527-1 | 6 | % | |
Izod Impact Strength | 没Notched | ISO 179 | NB | KJ/m |
带Notched | ISO 179 | 89 | KJ/m | |
Flexural Modulus | ISO178 | 2200 | Mpa | |
Flexural Stress | ISO178 | 90.0 | Mpa | |
Tensile Stress | Yield | ISO527-2/50 | 60.0 | Mpa |
Tensile Strain | Yield | ISO527-2/50 | 6.0 | % |
Tensile Stress(Yield) | ISO 527-1 | 60 | Mpa | |
Tensile Modulus | ASTM D638/ISO 527 | 2400 | kg/cm²(MPa)[Lb/in²] | |
ISO527-2/1 | 2350 | Mpa | ||
ISO 527-1 | 2350 | Mpa | ||
Tensile Elongation | Break | ISO 527-1 | >50 | % |
ASTM D638/ISO 527 | 6 | % | ||
Flexural Modulus | ASTM D790/ISO 178 | 2200 | kg/cm²(MPa)[Lb/in²] | |
ISO 178 | 2200 | Mpa | ||
Flexural Strength | ASTM D790/ISO 178 | 90 | kg/cm²(MPa)[Lb/in²] | |
Tensile Elongation?(Break) | ASTM D638/ISO 527 | >50 | % | |
Izod notch impact strength | ASTM D256/ISO 179 | 89 | kg·cm/cm(J/M)ft·lb/in |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Vicat Softening Temperature | ISO306/B50 | 151 | °C | |
Linear thermal expansion coefficient | MD | ISO11359-2 | 7E-05 | cm/cm/°C |
TD | ISO11359-2 | 7E-05 | cm/cm/°C | |
RTIElec | 1.5mm | UL746 | 125 | °C |
Evolution Calendar intelligent importer | 1.5mm | UL746 | 115 | °C |
RTIStr | 1.5mm | UL746 | 125 | °C |
Coefficient of Linear Thermal Expansion | ISO 11359-2 | 0.7 | ||
Deflection Temperature Under Load? | 1.80MPa | ISO 75-1 | 132 | °C |
ASTM D648/ISO 75 | 145 | ℃(℉) | ||
0.45MPa,Unannealed | ISO75-2/B | 145 | °C | |
1.8MPa,Unannealed | ISO75-2/A | 132 | °C | |
Vicat Softening Temperature | ASTM D1525/ISO R306 | 151 | ℃(℉) | |
ISO 306 | 151 | °C | ||
Linear expansion coefficient | ASTM D696/ISO 11359 | 0.7 | mm/mm.℃ | |
Flame retardancy | UL94 | HB |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Surface Resistivity | IEC60093 | >1.0E+15 | ohms | |
IEC 60093 | >1×10 | Ω | ||
ASTM D257/IEC 60093 | >1×10 15 | Ω | ||
Dielectric Constant | ASTM D150/IEC 60250 | 3 | ||
ASTM D150/IEC 60250 | 3.1 | |||
-,100HZ | IEC 60250 | 3.1 | ||
-,1MHz | IEC 60250 | 3 | ||
Arc Resistance | ASTM D495/IEC 60112 | 30 | ||
Volume Resistivity | ASTM D257/IEC 60093 | >1×10 13 | Ω.cm | |
IEC 60093 | >1×10 | Ω.m | ||
IEC60093 | >1.0E+15 | ohms·cm | ||
Relative Permittivity | 100Hz | IEC60250 | 3.10 | |
1MHz | IEC60250 | 3.00 | ||
Comparative Tracking Index | IEC60112 | 250 | V | |
Dielectric Strength | IEC60243-1 | 30 | KV/mm | |
Dissipation Factor? | 100Hz | IEC60250 | 1E-03 | |
1MHz | IEC60250 | 9E-03 | ||
Dissipation Factor?(Tangent) | -,100HZ | IEC 60250 | 10 | |
-,1MHZ | IEC 60250 | 90 |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Unnotched Impact Strength | ISO179 | NoBreak |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Transmittance | 3000µm | ASTMD1003 | 88.0 | % |
Transmittance | 3mm厚 | ASTM D1003 | 88 | % |
ASTM D1003/ISO 13468 | 88 | % | ||
Refractive index of light | ASTM D542/ISO 489 | 1.585 | ||
ASTMD542 | 1.585 |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 0.38mm | UL94 | HB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.