PC LEXAN™ 153R-111 SABIC INNOVATIVE NANSHA
60
- Unit Price:
- $2924 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 30MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:UV resistance
- Application Areas:Automotive sector Lighting fixtures
- Color:--
- Grade:Weather resistant grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:3.20mm | 内部方法 | 0.50to0.70 | % |
Moisture Absorption | 24hr | ASTMD570 | 0.15 | % |
Equilibrium,23°C | ASTMD570 | 0.35 | % | |
Equilibrium,100°C | ASTMD570 | 0.58 | % | |
Melt Mass-Flow Rate | 300°C/1.2kg | ASTMD1238 | 2.5 | g/10min |
Specific Volume | ASTMD792 | 0.835 | cm³/g |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flexural Modulus | 50.0mmSpan | ASTMD790 | 2340 | Mpa |
Flexural Strength | Yield,50.0mmSpan | ASTMD790 | 93.1 | Mpa |
Taber Abrasion Resistance | 1000Cycles,1000g,CS-17Wheel | ASTMD1044 | 10.0 | mg |
Tensile Strength | Yield | ASTMD638 | 62.1 | Mpa |
Break | ASTMD638 | 65.5 | Mpa | |
Tensile Elongation | Yield | ASTMD638 | 7.0 | % |
Break | ASTMD638 | 110 | % |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Specific Heat | ASTMC351 | 1260 | J/kg/°C | |
Thermal Conductivity | ASTMC177 | 0.19 | W/m/K | |
Deflection Temperature Under Load? | 0.45MPa,Unannealed,6.40mm | ASTMD648 | 138 | °C |
1.8MPa,Unannealed,6.40mm | ASTMD648 | 132 | °C | |
Linear thermal expansion coefficient | MD:-40to95°C | ASTME831 | 6.8E-05 | cm/cm/°C |
Vicat Softening Temperature | ASTMD15255 | 157 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dielectric Strength | 3.20mm,inAir | ASTMD149 | 15 | KV/mm |
Dielectric Constant | 50Hz | ASTMD150 | 3.17 | |
60Hz | ASTMD150 | 3.17 | ||
1MHz | ASTMD150 | 2.96 | ||
Volume Resistivity | ASTMD257 | >1.0E+16 | ohms·cm | |
Dissipation Factor? | 50Hz | ASTMD150 | 9E-04 | |
60Hz | ASTMD150 | 9E-04 | ||
1MHz | ASTMD150 | 0.010 |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Gardner Impact | 23°C | ASTMD3029 | 169 | J |
Tensile Impact Strength | ASTMD1822 | 630 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell Hardness | M-Sale | ASTMD785 | 70 | |
R-Sale | ASTMD785 | 118 |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Refractive index of light | ASTMD542 | 1.586 | ||
Transmittance | 2540µm | ASTMD1003 | 88.0 | % |
Haze | 2540µm | ASTMD1003 | 1.0 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.