Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Moisture Absorption | 24 hr | ASTM D570 | 0.15 | % |
Moisture Absorption | Equilibrium, 23°C | ASTM D570 | 0.35 | % |
Moisture Absorption | Equilibrium, 100°C | ASTM D570 | 0.58 | % |
Specific Volume | | ASTM D792 | 0.830 | cm³/g |
Melt Mass-Flow Rate | 300°C/1.2 kg | ASTM D1238 | 11 | g/10 min |
Modeling Shrinkage - Flow | 3.20 mm | 内部方法 | 0.50 到 0.70 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Strength | Yield | ASTM D638 | 62.0 | Mpa |
Tensile Strength | Break | ASTM D638 | 68.0 | Mpa |
Tensile Elongation | Yield | ASTM D638 | 7.0 | % |
Tensile Elongation | Break | ASTM D638 | 130 | % |
Taber Abrasion Resistance | 1000 Cycles, 1000 g, CS-17 Wheel | ASTM D1044 | 10.0 | mg |
Flexural Modulus | 50.0 mm Span | ASTM D790 | 2340 | Mpa |
Flexural Strength | Yield, 50.0 mm Span | ASTM D790 | 97.0 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
RTI | | UL 746 | 130 | °C |
RTI Imp | | UL 746 | 130 | °C |
RTI Elec | | UL 746 | 130 | °C |
Specific Heat | | ASTM C351 | 1250 | J/kg/°C |
Thermal Conductivity | | ASTM C177 | 0.19 | W/m/K |
Deflection Temperature Under Load? | 0.45 MPa, Unannealed, 6.40 mm | ASTM D648 | 137 | °C |
Deflection Temperature Under Load? | 1.8 MPa, Unannealed, 6.40 mm | ASTM D648 | 132 | °C |
Coefficient of Linear Thermal Expansion (Flow) | -40 to 95°C | ASTM E831 | 6.8E-5 | cm/cm/°C |
Vicat Softening Temperature | | ASTM D15255 | 154 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
High Amp Arc Ignition | | UL 746 | PLC 1 | |
High Voltage Arc Tracking Rate | | UL 746 | PLC 2 | |
Comparative Tracking Index | | UL 746 | PLC 2 | |
Hot-wire Ignition | | UL 746 | PLC 2 | |
Dielectric Constant | 60 Hz | ASTM D150 | 3.17 | |
Dielectric Constant | 50 kHz | ASTM D150 | 3.17 | |
Dielectric Constant | 1 MHz | ASTM D150 | 2.96 | |
Volume Resistivity | | ASTM D257 | > 1.0E+17 | ohms·cm |
Dissipation Factor? | 50 Hz | ASTM D150 | 9.0E-4 | |
Dissipation Factor? | 60 Hz | ASTM D150 | 9.0E-4 | |
Dissipation Factor? | 1 MHz | ASTM D150 | 0.010 | |
Dielectric Strength | 3.20 mm, in Air | ASTM D149 | 15 | KV/mm |
Injection | Test Condition | Test Method | Test Result | Unit |
---|
Drying Time | | | 3.0 到 4.0 | hr |
Suggested Shot Size | | | 40 到 60 | % |
Rear Temperature | | | 270 到 295 | °C |
Middle Temperature | | | 280 到 305 | °C |
Front Temperature | | | 295 到 315 | °C |
Nozzle Temperature | | | 290 到 310 | °C |
Back Pressure | | | 0.300 到 0.700 | Mpa |
Screw Speed | | | 40 到 70 | rpm |
Vent Depth | | | 0.025 到 0.076 | mm |
Drying Temperature | | | 120 | °C |
Suggested Max Moisture | | | 0.020 | % |
Processing (Melt) Temp | | | 295 到 315 | °C |
Mold Temperature | | | 70 到 95 | °C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Gardner Impact | 23°C | ASTM D3029 | 169 | J |
Unnotched Izod Impact Strength | 23°C | ASTM D4812 | 3200 | J/m |
Tensile Impact Strength | | ASTM D1822 | 577 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell Hardness | M-Scale | ASTM D785 | 70 | |
Rockwell Hardness | R-Scale | ASTM D785 | 118 | |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|
Refractive index of light | | ASTM D542 | 1.586 | |
Haze | 2540 µm | ASTM D1003 | 1.0 | % |
Transmittance | 2540 µm | ASTM D1003 | 88.0 | % |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
Oxygen Index | | ASTM D2863 | 25 | % |
Flame Rating | 1.5 mm | UL 94 | HB | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.