Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | TD | ISO294-4 | 1.8 | % |
Modeling Shrinkage | MD | ISO294-4 | 2.0 | % |
Moisture Absorption | Saturation,23°C,2.00mm | ISO62 | 0.90 | % |
Moisture Absorption | Equilibrium,23°C,2.00mm,50%RH | ISO62 | 0.20 | % |
MediumDensity | | | 1.20 | g/cm³ |
Melt Mass-Flow Rate | | ISO1133 | 14 | g/10min |
Melt Volume flow Rate | 190°C/2.16kg | ISO1133 | 12.0 | cm3/10min |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Flexural Stress | 3.5%Strain | ISO178 | 85.0 | Mpa |
Tensile Stress | Yield | ISO527-2 | 73.5 | Mpa |
Tensile Strain | Yield | ISO527-2 | 13 | % |
Tensile Modulus | | ISO527-2 | 3350 | Mpa |
Flexural Modulus | | ISO178 | 3150 | Mpa |
Nominal Tensile Strain at Break | | ISO527-2 | 27 | % |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Deflection Temperature Under Load? | 0.45MPa,Unannealed | ISO75-2/B | 159 | °C |
Deflection Temperature Under Load? | 1.8MPa,Unannealed | ISO75-2/A | 103 | °C |
Linear thermal expansion coefficient | MD:-- | ISO11359-2 | 1E-04 | cm/cm/°C |
Linear thermal expansion coefficient | MD:-40to23°C | ISO11359-2 | 9E-05 | cm/cm/°C |
Linear thermal expansion coefficient | TD:-- | ISO11359-2 | 1E-04 | cm/cm/°C |
Linear thermal expansion coefficient | TD:-40to23°C | ISO11359-2 | 9E-05 | cm/cm/°C |
Linear thermal expansion coefficient | TD:AnnealingTemperature | ISO11359-2 | 160 | °C |
Linear thermal expansion coefficient | TD:AnnealingTime-Optional | ISO11359-2 | 30.0 | min/mm |
Melting Temperature | | ISO11357-3 | 178 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Dielectric Strength | | IEC60243-1 | 43 | KV/mm |
Dissipation Factor? | 100Hz | IEC60250 | 5E-04 | |
Dissipation Factor? | 1MHz | IEC60250 | 5.5E-03 | |
Relative Permittivity | 100Hz | IEC60250 | 3.90 | |
Relative Permittivity | 1MHz | IEC60250 | 3.80 | |
Comparative Tracking Index | | IEC60112 | 600 | V |
Surface Resistivity | | IEC60093 | >1.0E+15 | ohms |
Volume Resistivity | | IEC60093 | >1.0E+15 | ohms·cm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Charpy Unnotched Impact Strength | -30°C | ISO179/1eU | 230 | kJ/m² |
Charpy Unnotched Impact Strength | 23°C | ISO179/1eU | 250 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell Hardness | M-Sale | ISO2039-2 | 93 | |
Rockwell Hardness | R-Sale | ISO2039-2 | 121 | |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
FMVSS Flammability | | FMVSS302 | B | |
Fogging-G-value | condensate | ISO6452 | 3.5E-04 | g |
Burning Rate | 1.00mm | ISO3795 | <100 | mm/min |
Supplementary information | Test Condition | Test Method | Test Result | Unit |
---|
Emission | | VDA275 | <2.00 | mg/kg |
EmissionofOrganicCompounds | | VDA277 | 10.0 | µgC/g |
Odor | | VDA270 | 3.50 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.