Need Help? Contact Us service@plas.com
Get App

POM KOCETAL®  EL302 KOLON KOREA

46
  • Unit Price:
    $3420 USD/MT
  • Packaging Specification:
    25KG/PKG
  • Supply Quantity:
    60MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

serv********

For more detailed information including pricing, customization, and shipping, please contact supplier.

Technical Data Sheet

Physical PropertiesTest ConditionTest MethodTest ResultUnit
Modeling ShrinkageMDASTMD9551.8%
Modeling ShrinkageTDISO294-42.2%
Modeling ShrinkageMDISO294-42.2%
Moisture Absorption23°C,24hrISO620.63%
Moisture AbsorptionEquilibrium,23°C,60%RHASTMD5700.24%
Melt Mass-Flow Rate190°C/2.16kgASTMD12389.0g/10min
Melt Mass-Flow Rate190°C/2.16kgISO11339.0g/10min
Density / Specific GravityASTMD7921.38g/cm³
Density / Specific GravityISO11831.38g/cm³
Mechanical PropertiesTest ConditionTest MethodTest ResultUnit
Tensile StrengthYield,23°CASTMD63850.0Mpa
Flexural Stress23°CISO17870.0Mpa
Tensile StressYield,23°CISO527-254.0Mpa
Tensile StrainBreak,23°CISO527-2>50%
Tensile ElongationYield,23°CASTMD63880%
Flexural Modulus23°CASTMD7902000Mpa
Flexural Modulus23°CISO1782300Mpa
Flexural Strength23°CASTMD79072.0Mpa
Thermal PropertiesTest ConditionTest MethodTest ResultUnit
Deflection Temperature Under Load?0.45MPa,UnannealedASTMD648152°C
Deflection Temperature Under Load?1.8MPa,UnannealedASTMD64892.0°C
Deflection Temperature Under Load?1.8MPa,UnannealedISO75-2/A82.0°C
Linear thermal expansion coefficientMDASTMD6961.3E-04cm/cm/°C
Melting temperatureISO11357-3166°C
Melting temperature166°C
Electrical performanceTest ConditionTest MethodTest ResultUnit
Dielectric StrengthASTMD14919KV/mm
Dielectric StrengthIEC60243-119KV/mm
Surface ResistivityASTMD2571E+16ohms
Surface ResistivityIEC600931E+16ohms
Dielectric ConstantASTMD1503.70
Volume ResistivityASTMD2571E+14ohms·cm
Volume ResistivityIEC600931E+14ohms·cm
Dissipation Factor?1MHzASTMD1506E-03
Impact PropertiesTest ConditionTest MethodTest ResultUnit
Charpy Notched Impact Strength23°CISO179/1eA8.0kJ/m²
Notched Izod Impact Strength23°CASTMD25687J/m
hardnessTest ConditionTest MethodTest ResultUnit
Rockwell HardnessM-ScaleASTMD78578
Rockwell HardnessM-ScaleISO2039-288
FlammabilityTest ConditionTest MethodTest ResultUnit
UL flame retardant rating0.8mmUL94HB
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.