Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | MD1 | 内部方法 | 0.30到0.60 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Stress | Yield | ISO527-2/5 | 69.0 | Mpa |
Tensile Strain | Yield | ISO527-2/5 | 1.1 | % |
Tensile Modulus | | ISO527-2/1 | 7600 | Mpa |
Flexural Modulus | | ISO178 | 7000 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Linear thermal expansion coefficient | MD:23to60°C | ISO11359-2 | 3.1E-05 | cm/cm/°C |
Linear thermal expansion coefficient | TD:23to60°C | ISO11359-2 | 1.2E-04 | cm/cm/°C |
Heat Deflection Temperature | 1.8MPa,Unannealed,64.0mmSpan | ISO75-2/Af | 155 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Surface Resistivity | | ASTMD257 | 1.0E+2到1.0E+4 | ohms |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Notched Izod Impact Strength | 23°C | ISO180/1A | 5.0 | kJ/m² |
Unnotched Izod Impact Strength | 23°C | ISO180/1U | 20 | kJ/m² |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.