Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Moisture Absorption | 23C/50RH | ISO 62 | 0.20 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Modulus | 73℉ | ISO 527-1,-2 | 399000 | psi |
Breaking tensile strain | 73℉ | ISO 527-1,-2 | 24 | % |
Tensile Stress(Yield) | 73℉ | ISO 527-1,-2 | 9280 | psi |
Tensile Strain(Yield) | 73℉ | ISO 527-1,-2 | 7.5 | % |
Tensile Creep Modulus | 1000h | ISO 899-1 | 196000 | psi |
Charpy Notched Impact Strength | -22℉ | ISO 179 | 2.14 | ft·lb/in |
Charpy Notched Impact Strength | 73℉ | ISO 179 | 2.14 | ft·lb/in |
Charpy Unnotched Impact Strength | -22℉ | ISO 179 | 71.4 | ft·lb/in |
Charpy Unnotched Impact Strength | 73℉ | ISO 179 | 76.1 | ft·lb/in |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Flame retardancy | | UL94 | HB | |
Deflection Temperature Under Load? | 1.80MPa | ISO 75A-1,-2 | 203 | ℉ |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Volume Resistivity | | IEC 60093 | 1E+15 | ohm·cm |
Dissipation Factor? | 1E+6HZ,73℉ | IEC 60250 | 0.00500 | |
Surface resistance | | IEC 60093 | 1E+13 | ohms |
Processing | Test Condition | Test Method | Test Result | Unit |
---|
Processing temperature | | | 374-446 | ℉ |
Mold Temperature | | | 140-212 | ℉ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.