Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Melt Mass-Flow Rate | 190°C/2.16kg | ASTMD1238 | 2.0 | g/10min |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Coefficient of Friction | Dynamic,Blown Film | ASTMD1894 | 0.090 | |
Coefficient of Friction | Static,Blown Film | ASTMD1894 | 0.11 | |
Film | Test Condition | Test Method | Test Result | Unit |
---|
Elmendorf Tear Strength | MD:25μm,Blown Film | ASTMD1922 | 170 | g |
Elmendorf Tear Strength | TD:25μm,Blown Film | ASTMD1922 | 630 | g |
Gardner Impact | 25μm,Blown Film | ASTMD1709 | 61 | g |
Film Thickness - Tested) | | | 25 | µm |
Secant Modulus | 1%Secant,MD:25μm,Blown Film | ASTMD882 | 181 | Mpa |
Secant Modulus | 1%Secant,TD:25μm,Blown Film | ASTMD882 | 192 | Mpa |
Tensile Strength | MD:Yield,25μm,Blown Film | ASTMD882 | 9.00 | Mpa |
Tensile Strength | TD:Yield,25μm,Blown Film | ASTMD882 | 9.00 | Mpa |
Tensile Strength | MD:Break,25μm,Blown Film | ASTMD882 | 14.0 | Mpa |
Tensile Strength | TD:Break,25μm,Blown Film | ASTMD882 | 13.0 | Mpa |
Tensile Elongation | MD:Yield,25μm,Blown Film | ASTMD882 | 51 | % |
Tensile Elongation | TD:Yield,25μm,Blown Film | ASTMD882 | 21 | % |
Tensile Elongation | MD:Break,25μm,Blown Film | ASTMD882 | 570 | % |
Tensile Elongation | TD:Break,25μm,Blown Film | ASTMD882 | 560 | % |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|
Gloss | 45°,25.0μm,Blown Film | ASTMD2457 | 70 | |
Haze | 25.0μm,Blown Film | ASTMD1003 | 16 | % |
Supplementary information | Test Condition | Test Method | Test Result | Unit |
---|
Blow-upRatio | | | 2.00到4.00 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.