Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Instrumented Dart Impact | | ASTM D-2457 | 120 | g |
Elmendorf Tear Strength | MD | ASTM D-1922 | 5 | g/μm |
Elmendorf Tear Strength | TD | ASTM D-1922 | 9 | g/μm |
Tensile Strength (Break) | MD | ASTM D-882 | 400 | kg/cm2 |
Tensile Strength (Break) | TD | ASTM D-882 | 330 | kg/cm2 |
Tensile Elongation (Break) | | ASTM D-882 | 850 | % |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Vicat Softening Temperature | | ASTM D-1525 | 102 | °C |
Other | Test Condition | Test Method | Test Result | Unit |
---|
Haze | | ASTM D-1003 | 17 | % |
Film Thickness | | HPC | 40 | μm |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|
Gloss | 45℃ | ASTM D-2457 | 72 | |
Physical | Test Condition | Test Method | Test Result | Unit |
---|
Density / Specific Gravity | | ASTM D-1505 | 0.920 | g/cm³ |
Melt Mass-Flow Rate | | ASTM D-1238 | 2 | g/10min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.