Technical Data Sheet
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Elongation (Break MD) | 40um | ISO 527-3 | 300 | % |
Tensile Elongation (Break TD) | 40um | ISO 527-3 | 500 | % |
Elmendorf Tear Strength (TD) | 40um | ISO 6383-2 | 2 | N |
Elmendorf Tear Strength (MD) | 40um | ISO 6383-2 | 4 | N |
Tensile Strength (MD) | 40um | ISO 527-3 | 20 | Mpa |
Tensile Strength (TD) | 40um | ISO 527-3 | 24 | Mpa |
Secant Modulus | 40um | ASTM D-882 | 200 | Mpa |
Gardner Impact | 40um | ISO 7765-1 | 130 | g |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Vicat Softening Temperature | | ISO 306/A50 | 96 | °C |
Melting temperature | | ISO 3146 | 111 | °C |
Processing | Test Condition | Test Method | Test Result | Unit |
---|
Melt Temperature | | | 160-190 | °C |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|
Haze | 1020um | ASTM D-1003 | 12 | % |
Gloss | 1020um | ASTM D-2457 | 75 | |
Physical | Test Condition | Test Method | Test Result | Unit |
---|
Density | | ISO 1183 | 0.921 | g/m3 |
Melt Mass-Flow Rate | 190℃/2.16kg | ISO 1133 | 0.7 | g/10min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.