Technical Data Sheet
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Strength(Break) | @厚 150μ(5.9mil) | ASTM D-882 | 纵向,横向,24,22 | Mpa |
Tensile Strength(Yield) | @厚 150μ(5.9mil) | ASTM D-882 | 纵向,横向,12,11 | Mpa |
Instrumented Dart Impact | F50 | ASTM D-1709A | 320 | g |
Flexural Modulus - 1% Secant | @厚 150μ(5.9mil) | ASTM D-882 | 纵向,横向,210,240 | Mpa |
Elmendorf Tear Strength | | ASTM D-1922 | 纵向,横向,400,750 | g |
Tensile Elongation?(Break) | @厚 150μ(5.9mil) | ASTM D-882 | 纵向,横向,500,650 | % |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Melting Temperature | | 埃克森美孚方法 | 109 | °C |
Other | Test Condition | Test Method | Test Result | Unit |
---|
anti-sticking agent | | | 否 | |
slip additive | | | 否 | |
heat stabilizer | | | 有 | |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|
Gloss | Across Flow,45° | ASTM D-2457 | 54 | % |
Haze | | ASTM D-1003 | 11.2 | % |
Physical | Test Condition | Test Method | Test Result | Unit |
---|
Density / Specific Gravity | | 埃克森美孚方法 | 0.922 | g/cm³ |
Melt index | | ASTM D-1238 | 0.33 | g/10min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.