Technical Data Sheet
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Strength | | GB 1040 | 20.3 | Mpa |
Tensile Elongation | Break | GB 1040 | 640 | % |
Environmental Stress Cracking Resistance | 48h | YD/T760-95 | 0/10 | 失效数 |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Brittleness Temperature | -76℃ | GB 5470 | 0/10 | 失效数 |
Environmental Stress Cracking Resistance | 96h | YD/T760-95 | 0/9 | 失效数 |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Volume Resistivity | | GB 1410 | 3.16×1014 | Ω·M |
Dielectric Constant | 1MHZ | GB 1409 | 2.3 | |
Dissipation Factor? | 1MHZ | GB 1409 | 1.54×10-4 | |
Other | Test Condition | Test Method | Test Result | Unit |
---|
Color | | YD/T760-95 | 本色 | |
浸水稳定性 | | GB 1409 | 合格 | |
Oxygen Transmission Rate | | GB 2951.37 | 146 | min |
Physical | Test Condition | Test Method | Test Result | Unit |
---|
Melt index | | GB 3682 | 0.8 | g/10min |
Density | | GB 1033 | 0.942 | g/cm³ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.