PMMA ACRYPET™  TF8 MITUBISHI RAYON JAPAN

52
  • Unit Price:
    $2965 USD/MT
  • Packaging Specification:
    25KG/PKG
  • Supply Quantity:
    26.6MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

serv********

For more detailed information including pricing, customization, and shipping, please contact supplier.

Technical Data Sheet

Physical PropertiesTest ConditionTest MethodTest ResultUnit
Haze3mmISO 147820.3%
Refractive index of lightNISO 4891.49
Light Transmittance3mmISO 13468-193%
Mechanical PropertiesTest ConditionTest MethodTest ResultUnit
Notched Izod Impact Strength1AJIS K71101.6KJ/m
tensile strength1A/5ISO 527-259Mpa
Tensile Elongation1A/1ISO 527-23.3GPa
Flexural StrengthISO 17890Mpa
Notched Izod Impact Strength1eU 无槽口JIS K711121KJ/m
Notched Izod Impact Strength1eA V槽口JIS K71111.2KJ/m
Tensile Elongation1A/5ISO 527-25%
Rockwell HardnessISO 2039101M Scale
Flexural ModulusISO 1783.3GPa
Thermal PropertiesTest ConditionTest MethodTest ResultUnit
Deflection Temperature Under Load 1.80MPaISO 75-295°C
Coefficient of Linear Thermal ExpansionJIS K71976×101/℃
Vicat Softening Temperature50NISO 306102°C
Melt index230℃,37.3NISO 113310g/10min
Specific HeatJIS K71231.5J/(g?℃)
Spiral Flow厚薄2mm,230℃三菱丽阳法220mm
Spiral Flow厚薄2mm,250℃三菱丽阳法340mm
Thermal ConductivityJIS A14120.2W/(m?℃)
Electrical performanceTest ConditionTest MethodTest ResultUnit
Volume ResistivityJIS K6911>10Ωm
Dissipation Factor60HzJIS K69110.05
Insulation Resistance4kV/secJIS K691120MV/m
Surface ResistivityJIS K6911>10Ω
Dielectric Constant60HzJIS K69113.7
Arc ResistanceJIS K6911没有痕迹
PhysicalTest ConditionTest MethodTest ResultUnit
Moisture Absorption24hrISO 620.3%
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.