Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Moisture Absorption | | ISO 62 | 2.1 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Modulus | | ISO 527-1/1A/1 | 2500 | Mpa |
Tensile Strain (Yield) | | ISO 527-2/1A/50 | 5 | % |
Tensile Stress (Yield) | | ISO 527-2/1A/50 | 65 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Ball PressureTest | (60°C) | IEC 60695-10-2 | 通过 | |
Vicat Softening Temperature | -- | ISO 306/B50 | 215 | °C |
Vicat Softening Temperature | -- | ISO 306/A50 | 230 | °C |
Deflection Temperature Under Load? | 0.45 MPa, Unannealed | ISO 75-2/Bf | 170 | °C |
Deflection Temperature Under Load? | 1.8 MPa, Unannealed | ISO 75-2/Af | 60 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Comparative Tracking Index | | IEC 60112 | 600 | V |
Surface Resistivity | | IEC 60093 | > 1.0E+15 | ohms |
Volume Resistivity | | IEC 62631-3-1 | > 1.0E+13 | ohms·m |
Injection | Test Condition | Test Method | Test Result | Unit |
---|
Drying Temperature | | | 80 | |
Suggested Max Moisture | | | 0.040 到 0.10 | |
Processing (Melt) Temp | | | 270 到 290 | |
Mold Temperature | | | 60 到 100 | |
Drying Time | | | 3.0 到 4.0 | |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Charpy Unnotched Impact Strength | -30°C | | 无断裂 | |
Charpy Unnotched Impact Strength | 23°C | | 无断裂 | |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Ball PressureTest (H 358/30) | | ISO 2039-1 | 110 | Mpa |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
Glow Wire Flammability Index | 1.5 mm | | 600 | °C |
Glow Wire Flammability Index | 3.0 mm | | 600 | °C |
Burning Rate | 2.00 mm | ISO 3795 | 30 | mm/min |
Burning Rate | 2.00 mm | FMVSS 302 | 30 | mm/min |
Flammability level | 0.75 mm | | HB | |
Flammability level | 1.5 mm | | HB | |
Flammability level | 3.0 mm | | HB | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.