PA66 LNP™ LUBRILOY™ RF206-BK1B605 SABIC INNOVATIVE US
91
- Unit Price:
- $3497 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:UV resistance Thermal stability
- Application Areas:Textile application Home appliance components
- Color:--
- Grade:--
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:24hr | ASTMD955 | 0.60 | % |
TD:24hr | ASTMD955 | 1.2 | % | |
Moisture Absorption | 24hr,50%RH | ASTMD570 | 0.38 | % |
Equilibrium,23°C,50%RH | ISO62 | 0.66 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Stress | Break | ISO527-2/5 | 118 | Mpa |
Tensile Strain | Break | ISO527-2/5 | 2.3 | % |
Flexural Stress | ISO178 | 167 | Mpa | |
Coefficient of Friction | Static | ASTMD3702Modified | 0.40 | |
Dynamic | ASTMD3702Modified | 0.40 | ||
Tensile Modulus | ASTMD638 | 8770 | Mpa | |
Tensile Strength | Break | ASTMD638 | 121 | Mpa |
Flexural Modulus | 50.0mmSpan | ASTMD790 | 7060 | Mpa |
Tensile Modulus | ISO527-2/1 | 8470 | Mpa | |
Tensile Elongation | Break | ASTMD638 | 2.5 | % |
Flexural Modulus | ISO178 | 7200 | Mpa | |
Flexural Strength | Break,50.0mmSpan | ASTMD790 | 173 | Mpa |
Specific Wear Rate | ASTMD3702Modified | 45.0 | 10^-10in^5-min/ft-lb-hr |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Heat Deflection Temperature | 1.8MPa,Unannealed,64.0mmSpan | ISO75-2/Af | 224 | °C |
0.45MPa,Unannealed,64.0mmSpan | ISO75-2/Bf | 252 | °C | |
Deflection Temperature Under Load? | 0.45MPa,Unannealed,3.20mm | ASTMD648 | 258 | °C |
1.8MPa,Unannealed,3.20mm | ASTMD648 | 241 | °C | |
Linear thermal expansion coefficient | MD:-30to30°C | ASTMD696 | 3.8E-05 | cm/cm/°C |
TD:-30to30°C | ASTMD696 | 7.5E-05 | cm/cm/°C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Instrumented Dart Impact | 23°C,TotalEnergy | ASTMD3763 | 13.3 | J |
Multi-Axial Instrumented Impact Energy | ISO6603-2 | 3.70 | J | |
Notched Izod Impact Strength | 23°C | ISO180/1A | 9.1 | kJ/m² |
Unnotched Izod Impact Strength | 23°C | ISO180/1U | 35 | kJ/m² |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.