PA66 AKROMID® A3GK30 AKRO-PLASTIC GERMANY
160
- Unit Price:
- $3527 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 20MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Excellent appearance Glass bead reinforcement Low warpage enhance 30% Filler by weight Filler: Glass beads
- Application Areas:Electrical field Electrical appliances Electronic field Household appliances Shell
- Color:--
- Grade:--
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | TD | ISO294-4 | 1.3 | % |
MD | ISO294-4 | 1.2 | % | |
Moisture Absorption | Saturation,23°C | ISO62 | 5.8 | % |
HumidityAbsorption-62%RH | 70°C | ISO1110 | 2.0 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flexural Strain (Break) | ISO178 | 6.5 | % | |
Flexural Modulus | ISO178 | 4300 | Mpa | |
Flexural Stress | ISO178 | 140 | Mpa | |
Tensile Stress | Break | ISO527-2/5 | 90.0 | Mpa |
Tensile Strain | Break | ISO527-2/5 | 4.0 | % |
Tensile Modulus | ISO527-2/1 | 5000 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 0.45MPa,Unannealed | ISO75-2/B | 225 | °C |
1.8MPa,Unannealed | ISO75-2/A | 100 | °C | |
Melting Temperature | DINEN11357-1 | 262 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Comparative Tracking Index | SolutionA | IEC60112 | 500 | V |
Surface Resistivity | IEC60093 | 1E+13 | ohms | |
Volume Resistivity | IEC60093 | 1E+15 | ohms·cm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Unnotched Impact Strength | -30°C | ISO179/1eU | 22 | kJ/m² |
23°C | ISO179/1eU | 28 | kJ/m² |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flame Rating | 1.6mm | UL94 | HB | |
Burning Rate | 1.00mm | FMVSS302 | <100 | mm/min |
GlowWireFlammability | 1.6mm | IEC60695-2-12 | 650 | °C |
Supplementary information | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
ReinforcementContent | ISO1172 | 30 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.