Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Moisture Absorption | 24 hr, 23°C | ASTM D570 | 1.7 | % |
Modeling Shrinkage - Flow | 23°C, Injection | ASTM D955 | 1.3 到 2.0 | % |
Density / Specific Gravity | | ASTM D792 | 1.14 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Elongation | Break, 23°C, 3.20 mm, Injection | ASTM D638 | > 40 | % |
Flexural Modulus | 23°C, 3.20 mm, Injection | ASTM D790 | 2550 | Mpa |
Flexural Strength | 23°C, 3.20 mm, Injection | ASTM D790 | 102 | Mpa |
Tensile Strength | Break, 23°C, 3.20 mm, Injection | ASTM D638 | 74.5 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Peak Melting Temperature | | ASTM D3418 | 260 | °C |
Deflection Temperature Under Load? | 0.45 MPa, Unannealed, 6.40 mm, Injection | ASTM D648 | 230 | °C |
Deflection Temperature Under Load? | 1.8 MPa, Unannealed, 6.40 mm, Injection | ASTM D648 | 75.0 | °C |
Injection | Test Condition | Test Method | Test Result | Unit |
---|
Drying Time | | | 4.0 到 5.0 | hr |
Rear Temperature | | | 255 到 270 | °C |
Middle Temperature | | | 260 到 275 | °C |
Front Temperature | | | 260 到 275 | °C |
Nozzle Temperature | | | 260 到 280 | °C |
Drying Temperature | | | 80 到 100 | °C |
Suggested Max Moisture | | | 0.10 | % |
Processing (Melt) Temp | | | 260 到 280 | °C |
Mold Temperature | | | 60 到 90 | °C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Notched Izod Impact Strength | 23°C, 6.40 mm, Injection | ASTM D256 | 49 | J/m |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
Flame Rating | 0.70 mm | UL 94 | V-2 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.