PA66 LNP™ LUBRICOMP™ RFL36 SABIC INNOVATIVE US
100
- Unit Price:
- $5475 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 65MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:wear resistant Thermal stability Filler: Glass fiber reinf 30% filler by weight
- Application Areas:Electronic display
- Color:--
- Grade:Extrusion grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:24hr | ASTMD955 | 0.40to0.60 | % |
TD:24hr | ASTMD955 | 1.0to3.0 | % | |
Moisture Absorption | 24hr,50%RH | ASTMD570 | 0.37 | % |
Equilibrium,23°C,50%RH | ISO62 | 0.58 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Stress | Yield | ISO527-2/5 | 168 | Mpa |
Break | ISO527-2/5 | 158 | Mpa | |
Tensile Strain | Yield | ISO527-2/5 | 2.8 | % |
Break | ISO527-2/5 | 2.8 | % | |
Flexural Stress | ISO178 | 219 | Mpa | |
Coefficient of Friction | Dynamic | ASTMD3702Modified | 0.67 | |
Static | ASTMD3702Modified | 0.61 | ||
Tensile Elongation | Yield | ASTMD638 | 2.8 | % |
Specific Wear Rate | Ring | ASTMD3702Modified | 0.250 | 10^-10in^5-min/ft-lb-hr |
Washer | ASTMD3702Modified | 5.00 | 10^-10in^5-min/ft-lb-hr | |
Tensile Modulus | ASTMD638 | 11700 | Mpa | |
Tensile Strength | Break | ASTMD638 | 160 | Mpa |
Yield | ASTMD638 | 160 | Mpa | |
Flexural Modulus | 50.0mmSpan | ASTMD790 | 9260 | Mpa |
Flexural Strength | Yield,50.0mmSpan | ASTMD790 | 233 | Mpa |
Tensile Modulus | ISO527-2/1 | 10400 | Mpa | |
Tensile Elongation | Break | ASTMD638 | 2.8 | % |
Flexural Modulus | ISO178 | 8890 | Mpa | |
Flexural Strength | Break,50.0mmSpan | ASTMD790 | 233 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Heat Deflection Temperature | 1.8MPa,Unannealed,64.0mmSpan | ISO75-2/Af | 244 | °C |
0.45MPa,Unannealed,64.0mmSpan | ISO75-2/Bf | 258 | °C | |
Deflection Temperature Under Load? | 0.45MPa,Unannealed,3.20mm | ASTMD648 | 260 | °C |
1.8MPa,Unannealed,3.20mm | ASTMD648 | 249 | °C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Notched Izod Impact Strength | 23°C | ISO180/1A | 7.5 | kJ/m² |
Unnotched Izod Impact Strength | 23°C | ISO180/1U | 55 | kJ/m² |
Instrumented Dart Impact | 23°C,TotalEnergy | ASTMD3763 | 8.50 | J |
Multi-Axial Instrumented Impact Energy | ISO6603-2 | 2.50 | J |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.