PA66 Zytel® HTN-53G50LR-BN517 DUPONT JAPAN
84
- Unit Price:
- $3750 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 40.5MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Flame retardant Thermal stability High temperature resistan Glass fiber reinforced Filler: Glass fiber reinf 50% filler by weight
- Application Areas:Food containers
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | TD | ISO294-4 | 0.50 | % |
MD | ISO294-4 | 0.20 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Creep Modulus | 1000hr | ISO899-1 | -- | Mpa |
Tensile Stress | Break | ISO527-2 | 250 | Mpa |
Tensile Strain | Break | ISO527-2 | 2.8 | % |
Tensile Modulus | ISO527-2 | 16000 | Mpa | |
Flexural Modulus | ISO178 | 15000 | Mpa | |
Tensile Creep Modulus | 1hr | ISO899-1 | -- | Mpa |
Flexural Stress | ISO178 | 390 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melting Temperature | ISO11357-3 | 260 | °C | |
Linear thermal expansion coefficient | MD:-- | ISO11359-2 | 1.7E-05 | cm/cm/°C |
MD:-40to23°C | ISO11359-2 | 1.9E-05 | cm/cm/°C | |
TD:-- | ISO11359-2 | 5.9E-05 | cm/cm/°C | |
TD:-40to23°C | ISO11359-2 | 5.9E-05 | cm/cm/°C | |
TD:55to160°C | ISO11359-2 | 9.5E-05 | cm/cm/°C | |
Deflection Temperature Under Load? | 0.45MPa,Unannealed | ISO75-2/B | 254 | °C |
1.8MPa,Unannealed | ISO75-2/A | 234 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Volume Resistivity | IEC60093 | 1E+15 | ohms·cm | |
Comparative Tracking Index | IEC60112 | 550 | V |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Unnotched Impact Strength | -30°C | ISO179/1eU | 65 | kJ/m² |
23°C | ISO179/1eU | 95 | kJ/m² |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 0.75mm | UL94 | HB | |
1.5mm | UL94 | HB | ||
0.75mm | IEC60695-11-10,-20 | HB | ||
1.5mm | IEC60695-11-10,-20 | HB | ||
Oxygen Index | ISO4589-2 | 27 | % | |
FMVSS Flammability | FMVSS302 | B | ||
Burning Rate | 1.00mm | ISO3795 | <100 | mm/min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.