Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Melt Volume flow Rate | 275℃,5 kg | ISO 1133 | 40 | cm3/10min |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Modulus | | ISO 527 | 3200 | Mpa |
Tensile Strain | Yield | ISO 527 | 4.2 | % |
Tensile Strain | Break | ISO 527 | >50 | % |
Tensile Strength | Yield | ISO 527 | 85 | Mpa |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Charpy Unnotched Impact Strength | 23℃ | ISO 179/1eU | 未断裂 | kJ/m² |
Charpy Notched Impact Strength | 23℃ | ISO 179/1eA | 5.7 | kJ/m² |
Charpy Notched Impact Strength | -30℃ | ISO 179/1eA | 5 | kJ/m² |
Notched Izod Impact Strength | 23℃ | ISO 180-1eA | 6 | kJ/m² |
Notched Izod Impact Strength | -30℃ | ISO 180-1eA | 7 | kJ/m² |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
Flame Rating | 1.50 mm | UL 94 | V-2 | |
Thermal | Test Condition | Test Method | Test Result | Unit |
---|
Heat Deflection Temperature | 1.8 Mpa | ISO 75-1/2 | 75 | °C |
Heat Deflection Temperature | 0.45 MPa | ISO 75-1/2 | 220 | °C |
Melting Temperature | | ISO 11357-1/-3 | 260 | °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.