Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | MD | 内部方法 | 1.7to2.2 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Stress | Yield,23°C | ISO527-2 | 72.0 | Mpa |
Tensile Stress | Break,23°C | ISO527-2 | 64.0 | Mpa |
Tensile Strain | Yield,23°C | ISO527-2 | 4.5 | % |
Tensile Strain | Break,23°C | ISO527-2 | 15 | % |
Tensile Strength | | ASTMD638 | 70.0 | Mpa |
Flexural Stress | 23°C | ISO178 | 88.0 | Mpa |
Tensile Modulus | 23°C | ISO527-2 | 2400 | Mpa |
Tensile Elongation | Break | ASTMD638 | 20 | % |
Flexural Modulus | | ASTMD790 | 2500 | Mpa |
Flexural Modulus | 23°C | ISO178 | 2200 | Mpa |
Flexural Strength | | ASTMD790 | 98.0 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Deflection Temperature Under Load? | 0.45MPa,Unannealed | ASTMD648 | 225 | °C |
Deflection Temperature Under Load? | 0.45MPa,Unannealed | ISO75-2/B | 209 | °C |
Deflection Temperature Under Load? | 1.8MPa,Unannealed | ASTMD648 | 77.0 | °C |
Deflection Temperature Under Load? | 1.8MPa,Unannealed | ISO75-2/A | 66.0 | °C |
Linear thermal expansion coefficient | MD | ASTMD696 | 7E-05 | cm/cm/°C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Charpy Unnotched Impact Strength | | ISO179 | NoBreak | |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell Hardness | R-Scale | ASTMD785 | 114 | |
Rockwell Hardness | R-Scale | ISO2039-2 | 114 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.