Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | MD:3.00mm | ASTMD955 | 0.20到0.40 | % |
Moisture Absorption | 23°C,24hr | ASTMD570 | 0.30 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Elongation | Break | ASTMD638 | 2.5 | % |
Flexural Modulus | | ASTMD542 | 8960 | Mpa |
Flexural Strength | | ASTMD542 | 241 | Mpa |
Tensile Strength | Yield | ASTMD638 | 152 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Deflection Temperature Under Load? | 1.8MPa,Unannealed | ASTMD648 | 210 | °C |
Peak Melting Temperature | | ASTMD789 | 220 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Dielectric Strength | | ASTMD149 | 26 | KV/mm |
Arc Resistance | | ASTMD495 | 130到140 | sec |
Volume Resistivity | | ASTMD257 | 2E+13 | ohms·cm |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell Hardness | R-Scale | ASTMD785 | 120 | |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
UL flame retardant rating | 3.2mm | UL94 | HB | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.