PA6 Grilon® BGZ-15/2 EMS-CHEMIE SWITZERLAND
99
- Unit Price:
- $3766 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 29.8MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Glass fiber reinforced Electrical performance Antichemical wear resistant Thermal stability High impact resistance high strength High hardness
- Application Areas:electrical machinery Electrical field Electronic field Industrial machinery Automotive sector Shell
- Color:--
- Grade:--
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Moisture Absorption | Saturation,23℃ Saturation, 73°F | ISO 62 | 8 | % |
Equilibrium,23℃,50% RH Equilibrium, 73°F, 50% RH | ISO 62 | 2 | % | |
Modeling Shrinkage | TD Across Flow | ISO 294-4 | 0.7 | % |
MD Flow | ISO 294-4 | 0.2 | % | |
Density | ISO 1183 | 1.18 | g/cm³ |
Electrical | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Surface Resistivity | IEC 60093 | -- | ohms | |
Comparative Tracking Index | IEC 60112 | -- | V | |
Volume Resistivity | IEC 60093 | 100000000000000 | ohms·cm | |
Dielectric Strength | IEC 60243-1 | 40 | KV/mm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Unnotched Impact Strength | -30℃ -30°C | ISO 179/1eU | 70 | kJ/m² |
23℃ 23°C | ISO 179/1eU | 75 | kJ/m² | |
Charpy Notched Impact Strength | -30℃ -30°C | ISO 179/1eA | 11 | kJ/m² |
23℃ 23°C | ISO 179/1eA | 20 | kJ/m² |
机械性能 | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Strength | Break Break | ISO 527-2 | 110 | Mpa |
Tensile Strain | Break Break | ISO 527-2 | 5 | % |
Tensile Modulus | ISO 527-2 | 5300 | Mpa |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flame Rating | 0.8 mm 0.8 mm | IEC 60695-11-10, -20 | HB |
Thermal | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Heat Deflection Temperature | 1.8 MPa,Unannealed 264 psi, Unannealed | ISO 75-2/A | 190 | °C |
8.0 MPa,Unannealed 1160 psi, Unannealed | ISO 75-2/C | 55 | °C | |
Coefficient of Linear Thermal Expansion | MD Flow | ISO 11359-2 | 0.000050 | 1/℃ |
TD Transverse | ISO 11359-2 | 0.00012 | 1/℃ | |
Continuous Use Temperature | -- -- 3 3 | ISO 2578 | 90.0 到 120 | °C |
-- -- 4 4 | 内部方法 | 160 | °C | |
Melting Temperature Melting Temperature 5 5 | ISO 11357-3 | 222 | °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.