Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | TD | ISO294-4 | 1.2 | % |
Modeling Shrinkage | MD | ISO294-4 | 0.70 | % |
Moisture Absorption | Saturation,23°C,2.00mm | ISO62 | 7.5 | % |
Moisture Absorption | Equilibrium,23°C,2.00mm,50%RH | ISO62 | 2.4 | % |
Melt Viscosity | 280°C,1000sec^-1 | ISO11443 | 300000 | mPa·s |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Poisson Ratio | | ISO527 | -- | |
Tensile Stress | Break | ISO527-2 | 100 | Mpa |
Tensile Strain | Break | ISO527-2 | 5.0 | % |
Tensile Modulus | | ISO527-2 | 5000 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Deflection Temperature Under Load? | 0.45MPa,Unannealed | ISO75-2/B | 215 | °C |
Deflection Temperature Under Load? | 1.8MPa,Unannealed | ISO75-2/A | 190 | °C |
Melting Temperature | | ISO11357-3 | 221 | °C |
Glass Transition Temperature | | ISO11357-2 | 60.0 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Dissipation Factor? | 100Hz | IEC60250 | 0.016 | |
Dissipation Factor? | 1MHz | IEC60250 | 0.016 | |
Comparative Tracking Index | | IEC60112 | 600 | V |
Volume Resistivity | | IEC60093 | 1E+15 | ohms·cm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Charpy Unnotched Impact Strength | 23°C | ISO179/1eU | 80 | kJ/m² |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
Oxygen Index | | ISO4589-2 | 25 | % |
FMVSS Flammability | | FMVSS302 | B | |
Burning Rate | 1.00mm | ISO3795 | <100 | mm/min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.